    					| 纳米结构金属材料的塑性变形制备技术* | 
  					 
  					  										
						陶乃镕( ), 卢柯 | 
					 
															
					| 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016 | 
					 
										
						 | 
					 
   										
    					| PREPARATION TECHNIQUES FOR NANO-STRUCTURED METALLIC MATERIALS VIA PLASTIC DEFORMATION | 
  					 
  					  					  					
						TAO Nairong( ), LU Ke | 
					 
															
						| Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 | 
					   
									 
				
				引用本文: 
				
								陶乃镕, 卢柯. 纳米结构金属材料的塑性变形制备技术*[J]. 金属学报, 2014, 50(2): 141-147.	
																												 																				Nairong TAO,
																												Ke LU. 
				PREPARATION TECHNIQUES FOR NANO-STRUCTURED METALLIC MATERIALS VIA PLASTIC DEFORMATION[J]. Acta Metall Sin, 2014, 50(2): 141-147.	                                                        				  
				
				
					
						
							
								
									
									
									
									
									 
          
          
            
             
			              
            
									            
									                
																																															
																| [1] | 
																 
															     Segal V M, Reznikov V I, Drobyshevkij A E, Kopylov V I. Russ Metall, 1981; 1: 99
															     																 | 
																	  
																																
																| [2] | 
																 
															     Segal V M, Reznikov V I, Pavlik D A, Malyshev V F. Processes of Plastic Transformation of Metals. Minsk: Navuka Teknika, 1984: 295
															     																 | 
																	  
																																
																| [3] | 
																 
															     Valiev R Z, Annales de Chimie. Science des Materiaux, 1996; 21: 369
															     																 | 
																	  
																																
																| [4] | 
																 
															     Smirnova N A, Levit V I, Pilyugin V I, Kuznetsov R I, Davydova L S, Sazonnova V A. Fiz Met Metalloved, 1986; 61: 1170
															     																 | 
																	  
																																
																| [5] | 
																 
															     Zhilyaev A P, Nurislamova G V, Kim B K, Baro M D, Szpunar J A, Langdon T G. Acta Mater, 2003; 51: 753
															     																 | 
																	  
																																
																| [6] | 
																 
															     Zhilyaev A P, Langdon T G. Prog Mater Sci, 2008; 53: 893
															     																 | 
																	  
																																
																| [7] | 
																 
															     Saito Y, Tsuji N, Utsunomiya H, Sakai T, Hong R G. Scr Mater, 1998; 39: 1221
															     																 | 
																	  
																																
																| [8] | 
																 
															     Hosseini S A, Manesh H D. Mater Des, 2009; 30: 2911
															     																 | 
																	  
																																
																| [9] | 
																 
															     Tsuji N, Saito Y, Lee S H, Minamino Y. 2nd Int Conf on Nanomaterials by Severe Plastic Deformation (SPD): Fundamentals Processing Applications, Vienna, Austria: Wiley-V C H Verlag Gmbh, 2003: 338
															     																 | 
																	  
																																
																| [10] | 
																 
															     Lu K, Lu J. J Mater Sci Technol, 1999; 15: 193
															     																 | 
																	  
																																
																| [11] | 
																 
															     Tao N R, Sui M L, Lu J, Lu K. Nanostruct Mater, 1999; 11: 433
															     																 | 
																	  
																																
																| [12] | 
																 
															     Tao N R, Wang Z B, Tong W P, Sui M L, Lu J, Lu K. Acta Mater, 2002; 50: 4603
															     																 | 
																	  
																																
																| [13] | 
																 
															     Tong W P, Tao N R, Wang Z B, Lu J, Lu K. Science, 2003; 31: 299
															     																 | 
																	  
																																
																| [14] | 
																 
															     Lu K, Lu J. Mater Sci Eng, 2004; 375: 38
															     																 | 
																	  
																																
																| [15] | 
																 
															     Li W L, Tao N R, Lu K. Scr Mater, 2008; 59: 546
															     																 | 
																	  
																																
																| [16] | 
																 
															     Fang T H, Li W L, Tao N R, Lu K. Science, 2011; 331: 1587
															     																 | 
																	  
																																
																| [17] | 
																 
															     Zhao W S, Tao N R, Guo J Y, Lu Q H, Lu K. Scr Mater, 2005; 53: 745
															     																 | 
																	  
																																
																| [18] | 
																 
															     Tao N R, Lu K. J Mater Sci Technol, 2007; 23: 771
															     																 | 
																	  
																																
																| [19] | 
																 
															     Li Y S, Tao N R, Lu K. Acta Mater, 2008; 56: 230
															     																 | 
																	  
																																
																| [20] | 
																 
															     Bay B, Hansen N. Mater Sci Eng, 1989; A113: 385
															     																 | 
																	  
																																
																| [21] | 
																 
															     Ananthan V S, Leffers T, Hughes D A. Scr Metall Mater, 1991; 25: 137
															     																 | 
																	  
																																
																| [22] | 
																 
															     Hansen N. Mater Sci Technol, 1990; 6: 1039
															     																 | 
																	  
																																
																| [23] | 
																 
															     Li B L, Godfrey A, Meng Q C, Liu Q. Acta Mater, 2004; 52: 1069
															     																 | 
																	  
																																
																| [24] | 
																 
															     Liu Q, Huang X, Lloyd D J, Hansen N. Acta Mater, 2002; 50: 3789
															     																 | 
																	  
																																
																| [25] | 
																 
															     Wang Y M, Chen M W, Sheng H W, Ma E. J Mater Res, 2002; 17: 3004
															     																 | 
																	  
																																
																| [26] | 
																 
															     Valiev R Z, Krasilnikov N A, Tsenev N K. 5th Int Symp on Plasticity of Metals and Alloys, Prague, Czechoslovakia: Elsevier Science Sa Lausanne, 1990: 35
															     																 | 
																	  
																																
																| [27] | 
																 
															     Valiev R Z, Korznikov A V, Mulyukov R R. Symp on Nanophase Materials, at the Emrs 1992 Fall Meeting of the European-Materials-Research-Soc, Strasbourg, France: Elsevier Science Sa Lausanne, 1992: 141
															     																 | 
																	  
																																
																| [28] | 
																 
															     Valiev R Z, Langdon T G. Prog Mater Sci, 2006; 51: 881
															     																 | 
																	  
																																
																| [29] | 
																 
															     Valiev R Z, Islamgaliev R K, Alexandrov I V. Prog Mater Sci, 2000; 45: 103
															     																 | 
																	  
																																
																| [30] | 
																 
															     Bridgman P W. J Appl Phys, 1943; 15: 273
															     																 | 
																	  
																																
																| [31] | 
																 
															     Jiang H G, Zhu Y T, Butt D P, Alexandrov I V, Lowe T C. Mater Sci Eng, 2000; A290: 128
															     																 | 
																	  
																																
																| [32] | 
																 
															     Sakai G, Horita Z, Langdon T G. Mater Sci Eng, 2005; A393: 344
															     																 | 
																	  
																																
																| [33] | 
																 
															     Zhang Y, Tao N R, Lu K. Acta Mater, 2011; 58: 6048
															     																 | 
																	  
																																
																| [34] | 
																 
															     Hong C S, Tao N R, Huang X, Lu K. Acta Mater, 2010; 58: 3103
															     																 | 
																	  
																																
																| [35] | 
																 
															     Xiao G H, Tao N R, Lu K. Scr Mater, 2011; 65: 119
															     																 | 
																	  
																																
																| [36] | 
																 
															     Lu K, Yan F K, Wang H T, Tao N R. Scr Mater, 2012; 66: 878
															     																 | 
																	  
																																
																| [37] | 
																 
															     Yan F K, Liu G Z, Tao N R, Lu K. Acta Mater, 2012; 60: 1059
															     																 | 
																	  
																																
																| [38] | 
																 
															     Wang H T, Tao N R, Lu K. Acta Mater, 2012; 60: 4027
															     																 | 
																	  
																																
																| [39] | 
																 
															     Huang F, Tao N R, Lu K. J Mater Sci Technol, 2011; 27: 1
															     																 | 
																	  
																																
																| [40] | 
																 
															     Luo Z P, Zhang H W, Hansen N, Lu K. Acta Mater, 2012; 60: 1322
															     																 | 
																	  
																																
																| [41] | 
																 
															     Zhu K Y, Vassel A, Brisset F, Lu K, Lu J. Acta Mater, 2004; 52: 4101
															     																 | 
																	  
																																
																| [42] | 
																 
															     Wang K, Tao N R, Liu G, Lu J, Lu K. Acta Mater, 2006; 54: 5281
															     																 | 
																	  
																																
																| [43] | 
																 
															     Sun H Q, Shi Y N, Zhang M X, Lu K. Acta Mater, 2007; 55: 975
															     																 | 
																	  
																																
																| [44] | 
																 
															     Zhang H W, Hei Z K, liu G, Lu J, Lu K. Acta Mater, 2003; 51: 1871
															     																 | 
																	  
																																
																| [45] | 
																 
															     Wu X, Tao N, Hong Y, Lu J, Lu K. Acta Mater, 2002; 50: 2075
															     																 | 
																	  
																																
																| [46] | 
																 
															     Tao N R, Wu X L, Sui M L, Lu J, Lu K. J Mater Res, 2004; 19: 1623
															     																 | 
																	  
																																
																| [47] | 
																 
															     Liu X C, Zhang H W, Lu K. Science, 2013; 342: 337
															     																 | 
																	  
																																
																| [48] | 
																 
															     Zener C, Hollomon J H. J Appl Phys, 1944; 15: 22
															     																 | 
																	  
																																
																| [49] | 
																 
															     Li Y S, Zhang Y, Tao N R, Lu K. Acta Mater, 2009; 57: 761
															     																 | 
																	  
																																
																| [50] | 
																 
															     Ashby M F. Philos Mag, 1970; 21: 399
															     																 | 
																	  
																																													 
									             
									           
             
			            			 
			 
             
												
											    	
											        	 | 
											        	Viewed | 
											         
													
											        	 | 
											        	 | 
											         
											      	
												         | 
												        
												        	Full text 
												          	
												         | 
											        	
												        	
												        	 
												        	
												          	 
												          	
												          	
														 | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        
												        	Abstract 
												          	
														 | 
												        
															
															 
															
															
												         | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        Cited  | 
												        
												        	
												         | 
													 
													
												         | 
												         | 
												         | 
													 
													
													    |   | 
													    Shared | 
													       | 
												  	 
												  	
													     | 
													     | 
													     | 
											  		 
											  		
													    |   | 
													    Discussed | 
													       | 
												  	 
											 
											 
             
           
      
									
									
		
									
									
									
									
									
									 | 
								 
							 
						 | 
					 
				 
			
		 |