| 1300 MPa级0.14C-2.72Mn-1.3Si钢的显微组织和力学性能及加工硬化行为 |
| 赵征志1,2, 佟婷婷1,2, 赵爱民1,2, 何青1,2, 董瑞1,2, 赵复庆1,2 |
1 北京科技大学冶金工程研究院, 北京 100083 2 北京科技大学现代交通先进金属材料与加工技术北京实验室, 北京 100083 |
|
| MICROSTRUCTURE, MECHANICAL PROPERTIES AND WORK HARDENING BEHAVIOR OF 1300 MPa GRADE 0.14C-2.72Mn-1.3Si STEEL |
| ZHAO Zhengzhi1,2, TONG Tingting1,2, ZHAO Aimin1,2, HE Qing1,2, DONG Rui1,2, ZHAO Fuqing1,2 |
1 Engineering Research Institute, University of Science and Technology Beijing, Beijing 100083 2 Beijing Laboratory of Modern Traffic Metal Materials and Processing Technology, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
赵征志, 佟婷婷, 赵爱民, 何青, 董瑞, 赵复庆. 1300 MPa级0.14C-2.72Mn-1.3Si钢的显微组织和力学性能及加工硬化行为[J]. 金属学报, 2014, 50(10): 1153-1162.
Zhengzhi ZHAO,
Tingting TONG,
Aimin ZHAO,
Qing HE,
Rui DONG,
Fuqing ZHAO.
MICROSTRUCTURE, MECHANICAL PROPERTIES AND WORK HARDENING BEHAVIOR OF 1300 MPa GRADE 0.14C-2.72Mn-1.3Si STEEL[J]. Acta Metall Sin, 2014, 50(10): 1153-1162.
| [1] |
Hayami S, Furukawa T. Microalloying 75. New York: Union Carbide Corp, 1977: 311
|
| [2] |
Matsumura O, Sakuma Y, Takechi H. Scr Metall, 1987; 21: 1301
|
| [3] |
Sugimoto K, Misu M, Kobayashi M, Shirasawa H. ISIJ Int, 1993; 33: 775
|
| [4] |
Bouaziz O, Guelton N. Mater Sci Eng, 2001 A319-321: 246
|
| [5] |
Barnett M R. Mater Sci Eng, 2007; A464: 1
|
| [6] |
Speer J G, Matlock D K, De Cooman B C, Schroth J G. Acta Mater, 2003; 51: 2611
|
| [7] |
Matlock D K, Brautigam V E, Speer J G. Mater Sci Forum, 2003; 426-432: 1089
|
| [8] |
Jiang H T, Tang D, Mi Z L, Chen Y L. J Univ Sci Technol Beijing, 2010; 32: 201
|
| [8] |
(江海涛, 唐 荻, 米振莉, 陈雨来. 北京科技大学学报, 2010; 32: 201)
|
| [9] |
Nouri A, Saghafian H, Kheirandish S. J Iron Steel Res Int, 2010; 17(5): 44
|
| [10] |
Fan Y, Wang M L, Zhang H, Tao H B, Zhao P, Li S Q. J Univ Sci Technol Beijing, 2013; 35: 607
|
| [10] |
(范 倚, 王明林, 张 慧, 陶红标, 赵 沛, 李士琦. 北京科技大学学报, 2013; 35: 607)
|
| [11] |
Zhong N, Wang X D, Wang L, Rong Y H. Mater Sci Eng, 2009; A506: 111
|
| [12] |
Li Z, Zhao A M, Tang D, Mi Z L, Jiao D H. J Univ Sci Technol Beijing, 2012; 34: 132
|
| [12] |
(李 振, 赵爱民, 唐 荻, 米振莉, 焦殿辉. 北京科技大学学报, 2012; 34: 132)
|
| [13] |
Zhang L Y, Wu D, Li Z. J Iron Steel Res Int, 2012; 19(2): 42
|
| [14] |
Koh-ichi S, Daiki F, Nobuo Y. Procedia Eng, 2010; 2: 359
|
| [15] |
Speich G R, Demarest V A, Miller R L. Metall Trans, 1981; 12A: 1419
|
| [16] |
Sayed A A, Kheirandish Sh. Mater Sci Eng, 2012; A532: 21
|
| [17] |
Rosenberg G, Sinaiová I, Juhar Ľ. Mater Sci Eng, 2013; A582: 347
|
| [18] |
Yan S, Liu X H, Liu W J, Lan H F, Wu H Y. Acta Metall Sin, 2013; 49: 917
|
| [18] |
(闫 述, 刘相华, 刘伟杰, 蓝慧芳, 吴红艳. 金属学报, 2013; 49: 917)
|
| [19] |
Wang C Y, Shi J, Cao W Q, Dong H. Acta Metall Sin, 2011; 47: 720
|
| [19] |
(王存宇, 时 捷, 曹文权, 董 瀚. 金属学报, 2011; 47: 720)
|
| [20] |
Mohammad R A, Ekrami A. Mater Sci Eng, 2008; A477: 30
|
| [21] |
Kang Y L, Kuang S, Yin X D. Automob Technol Mater, 2006; (5): 1
|
| [21] |
(康永林, 邝 霜, 尹显东. 汽车工艺与材料, 2006; (5): 1)
|
| [22] |
Ren Y Q, Xie Z J, Shang C J. Acta Metall Sin, 2012; 48: 1074
|
| [22] |
(任勇强, 谢振家, 尚成嘉. 金属学报, 2012; 48: 1074)
|
| [23] |
Li Y L. J Chongqing Univ (Nat Sci), 2001; 24(3): 58
|
| [23] |
(李玉兰. 重庆大学学报(自然科学版), 2001; 24(3): 58)
|
| [24] |
Colla V, Sanctis D M, Dimatteo A. Metall Mater Trans, 2009; 40: 2557
|
| [25] |
Nie W J, Shang C J, Guan H L, Zhang X B, Chen S H. Acta Metall Sin, 2012; 48: 298
|
| [25] |
(聂文金, 尚成嘉, 关海龙, 张晓兵, 陈少慧. 金属学报, 2012; 48: 298)
|
| [26] |
Zhao Z Z, Ye J Y, Wang Z G, Zhao A M. J Shenyang Univ Technol, 2013; 35: 36
|
| [26] |
(赵征志, 叶洁云, 汪志刚, 赵爱民. 沈阳工业大学学报, 2013; 35: 36)
|
| [27] |
Seyedrezai H, Pilkey A K, Boyd J D. Mater Sci Eng, 2014; A594: 178
|
| [28] |
Mazinani M, Poole W J. Metall Mater Trans, 2007; 38A: 328
|
| [29] |
Lanzillotto C A N, Pickering F B. Met Sci, 1982; 16: 371
|
| [30] |
Ashby M F. Philos Mag, 1966; 14: 1157
|
| [31] |
Ashby M F. Philos Mag, 1970; 21: 399
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|