| 热氧化法制备超疏水Ti表面及其耐腐蚀性 |
| 康志新,郭明杰 |
| 华南理工大学机械与汽车工程学院国家金属材料近净成形工程技术研究中心, 广州 510640 |
|
| FABRICATION OF SUPERHYDROPHOBIC Ti SURFACE BY THERMAL OXIDATION AND ITS ANTICORROSION PROPERTY |
| KANG Zhixin, GUO Mingjie |
| National Engineering Research Center of Near-Net-Shape Forming for Metallic Materials, School of Mechanical and Automotive Engineering, South China University of Technology, Guangzhou 510640 |
引用本文:
康志新,郭明杰. 热氧化法制备超疏水Ti表面及其耐腐蚀性[J]. 金属学报, 2013, 49(5): 629-634.
KANG Zhixin,
GUO Mingjie.
FABRICATION OF SUPERHYDROPHOBIC Ti SURFACE BY THERMAL OXIDATION AND ITS ANTICORROSION PROPERTY[J]. Acta Metall Sin, 2013, 49(5): 629-634.
| [1] Ou J F, Liu M Z, Li W, Wang F J, Xue M S, Li C Q. Appl Surf Sci, 2012; 258: 4724 [2] Zhang F, Chen S G, Dong L H, Lei Y H, Liu T, Yin Y S. Appl Surf Sci, 2011; 257: 2587 [3] Nakajima A, Hashimoto K, Watanabe T. Langmuir, 2000; 16: 7044 [4] Gao X, Jiang L. Nature, 2004; 432: 36 [5] Isimjan T T, Wang T, Rohani S. Chem Eng J, 2012; 210: 182 [6] Xu Q J, Deng X Q, Pan H T, Yun H. Acta Metall Sin, 2012; 48: 94 (徐群杰, 邓先钦, 潘红涛, 云虹. 金属学报, 2012; 48: 94) [7] He T, Wang Y C, Zhang Y J, Lv Q, Xu T G, Liu T. Corros Sci, 2009; 51: 1757 [8] Kang Z X, Lai X M, Sang J, Li Y Y. Thin Solid Films, 2011; 520: 800 [9] Xi J M, Feng L, Jiang L. Appl Phys Lett, 2008; 92: 53102 [10] Siva R K D, Sun Y. Surf Coat Technol, 2005; 198: 447 [11] Ashrafizadeh A, Ashrafizadeh F. J Alloys Compd, 2009; 480: 849 [12] Jiang L, Zhao Y, Zhai J. Angew Chem Int Ed, 2004; 116: 4438 [13] Hauffe K. Oxidation of Metals. New York: Plenum Press, 1965: 209 [14] Nakata K, Sakai M, Ochiai T, Murakami T, Takagi K, Fujishima A. Mater Lett, 2012; 70: 160 [15] Dong H, Li X Y. Mater Sci Eng, 2000; A280: 303 [16] Bhushan B, Her E K. Langmuir, 2010; 26: 8207 [17] Bhushan B, Jung Y C, Koch K. Langmuir, 2009; 25: 3240 [18] Nishino T, Meguro M, Nakamae K, Matsushita M, Ueda Y. Langmuir, 1999; 15: 4321 [19] Wenzel R N. Ind Eng Chem, 1936; 28: 988 [20] Cassie A B D, Baxter S. Trans Faraday Soc, 1944; 40: 546 [21] Wang S T, Feng L, Jiang L. Adv Mater, 2006; 18: 767 [22] Gao L, McCarthy T J. Langmuir, 2007; 23: 3762 [23] Gao L, McCarthy T J. Langmuir, 2006; 22: 2966 [24] Koga T, Morita M, Ishida H, Yakabe H, Sasaki S, Sakata O, Otsuka H, Takahara A. Langmuir, 2005; 21: 905 [25] Zhu X T, Zhang Z Z, Yang J, Xu X H, Men X H, Zhou X Y. J Colloid Interf Sci, 2012; 380: 182 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|