					引用本文:
						|  |  
    					|  |  
    					| Ti, C超过饱和固溶铝基复合薄膜的微结构和力学性能 |  
						| 尚海龙1, 2,沈洁1,杨铎1,孙士阳1,李戈扬1 |  
					| 1)上海交通大学金属基复合材料国家重点实验室, 上海 200240 2)上海电机学院机械学院, 上海 200245 |  
						|  |  
    					| MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Ti, C SOLID SOLUTION SUPERSATURATED Al-BASED COMPOSITE FILMS |  
						| SHANG Hailong 1, 2, SHEN Jie 1, YANG Duo 1, SUN Shiyang 1, LI Geyang 1 |  
						| 1)State Key Laboratory of Metal Matrix Composites, Shanghai Jiao Tong University, Shanghai 200240 2)School of Mechanical, Shanghai Dianji University, Shanghai 200245 |  
								尚海龙,沈洁,杨铎,孙士阳,李戈扬. Ti, C超过饱和固溶铝基复合薄膜的微结构和力学性能[J]. 金属学报, 2013, 49(3): 320-324.	
																												SHANG Hailong,
																								SHEN Jie,
																								YANG Duo,
																								SUN Shiyang,
																												LI Geyang. 
				MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Ti, C SOLID SOLUTION SUPERSATURATED Al-BASED COMPOSITE FILMS[J]. Acta Metall Sin, 2013, 49(3): 320-324.
 
					
						| 
								
									|  
          
          
            
                         
            
									            
									                
																														  
																| [1] Creus J, Berziou C, Cohendoz S, Perez A, Rebere C, Reffass M, Touzain S, Allely C, Gachon Y, Heau C,Sanchette F, Billard A.Corros Sci, 2012; 57: 162 [2] Leyland A, Matthews A.Surf Coat Technol, 2004; 177--178: 317 [3] Sanchette F, Ducros C, Billard A, Rebere C, Berziou C, Reffass M, Creus J.Thin Solid Films, 2009; 518: 1575 [4] Lewin E, Buchholt K, Lu J, Hultman L, Spetz L A, Jansson U.Thin Solid Films, 2010; 518: 5104 [5] Almtoft P K, Ejsing M A, Bφttiger J, Chevallier J.J Mater Res, 2007; 22: 1018 [6] El-Moneim A A, Akiyama E, Ismail M K, Hashimoto K.Corros Sci, 2011; 53: 2988 [7] Naka M, Maeda M, Shibayanagi T, Yuan H, Mori H.Vacuum, 2002; 65: 503 [8] Sanchette F, Billard A.Surf Coat Technol, 2001; 142: 218 [9] Perez A, Sanchette F, Billard A, Rebere C, Berziou C, Touzain S, Creus J.Mater Chem Phys, 2012; 132: 154 [10] Naka M, Shibayanag T, Maed M, Zhao S, Mori H.Vacuum, 2000; 59: 252 [11] Chandra T, Tsuzaki K, Militzer M, Ravindran C.Scr Mater, 2001; 44: 2035 [12] Boukhris N, Lallouche S, Debilia M Y, Draissia M.Eur Phys J Appl Phys, 2009; 45: 30501 [13] Draissia M, Boudemagh H, Debili Y M.Phys Scr, 2004; 69: 348 [14] Rupert J T, Trenkle C J, Schuh A C.Acta Mater, 2011; 59: 1619 [15] Mori M, Shibayanagi T, Maeda M, Naka M.Scr Mater, 2001; 44: 2035 [16] Mayrhofer H P, Mitterer C, Hultman L, Clemens H.Prog Mater Sci, 2006; 51: 1032 [17] Silva M, Wille C, Klement U, Choi P, Al-Kassab T.Mater Sci Eng, 2007; A445: 31 [18] Liu F.Appl Phys, 2005; 81A: 1095 [19] Pinkas M, Frage N, Froumin N, Pelleg J, Dariel M P.J Vac Sci Technol, 2002; 20A: 887 [20] Li X Y, Hua J D, Wang H Y, Guo Z X, Chumakov A N.Mater Sci Eng, 2007; A458: 235 [21] Meng Q P, Rong Y H, Hsu T Y.Mater Sci Eng, 2007; A471: 22 [22] Fleischer R L.The Strengthening of Metals. New York: Reinhold Publishing Corp, 1964: 93 [23] Labusch R.Phys Status Solidi, 1970; 41: 659 [24] Suzuki H.Dislocations and Mechanical Properties of Crystals. New York: Wiley, 1957: 361 [25] Meng Q P, Zhou N, Rong Y H, Chen S P, Hsu T Y (Xu Z Y).Acta Mater, 2002; 50: 4563 [26] Wu X L, Zhu Y T.Appl Phys, 2006; 89A: 031922 [27] Legros M, Gianola S D, Hemker J K.Acta Mater, 2008; 56: 3380   |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |