| 铜合金在中国南海深海环境下的腐蚀行为研究 |
| 孙飞龙,李晓刚,卢琳,万红霞,杜翠薇,刘智勇 |
| 北京科技大学腐蚀与防护中心, 北京100083 |
|
| CORROSION BEHAVIOR OF COPPER ALLOYS IN DEEP OCEAN ENVIRONMENT OF SOUTH CHINA SEA |
| SUN Feilong, LI Xiaogang, LU Lin, WAN Hongxia, DU Cuiwei, LIU Zhiyong |
| Corrosion and Protection Center, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
孙飞龙,李晓刚,卢琳,万红霞,杜翠薇,刘智勇. 铜合金在中国南海深海环境下的腐蚀行为研究[J]. 金属学报, 2013, 49(10): 1211-1218.
SUN Feilong,
LI Xiaogang,
LU Lin,
WAN Hongxia,
DU Cuiwei,
LIU Zhiyong.
CORROSION BEHAVIOR OF COPPER ALLOYS IN DEEP OCEAN ENVIRONMENT OF SOUTH CHINA SEA[J]. Acta Metall Sin, 2013, 49(10): 1211-1218.
| [1] David A, Shi X. Corros Sci, 2005; 47: 2335
[2] Zhou J L, Li X G, Cheng X Q, Dong C F, Du C W, Lu L. Corros Sci Prot Technol, 2010; 22: 47
(周建龙, 李晓刚, 程学群, 董超芳, 杜翠薇, 卢琳. 材料腐蚀与防护技术, 2010; 22: 47)
[3] Schumacher M. Sea Water Corrosion Handbook. New Jersey: Park Ridge, 1979: 150
[4] Dexter S C. Handbook of Oceanographic Engineering Materials. New York: Whiley-Interscience, 1979: 23
[5] Dexter S C. Corrosion, 1980; 36: 423
[6] Sparks C P, Cabillic J P, Schawann J C. J Energy Resour-Trans ASME, 1983; 105: 282
[7] Laque F L. Marine Corrosion. London: John Wiley and Sons Inc., 1975: 40
[8] Chandler K A. Marine and Offshore Corrosion (Marine Engineering Series). London: Butter worth, 1985: 72
[9] Warren A B. J Mar Res, 1982; 40: 823
[10] Sawant S S, Venkat K, Wagh A B. Indian J Technol, 1993; 31: 862
[11] Venkatesan R, Venkataswamy M A, Bhaskaran T A, Dwarakadasa E S, Ravindran M.Br Corros J, 2002; 37: 257
[12] Venkatesan R, Dwarakadasa E S, Ravindran M. Corros Prev Control, 2004; 51: 98
[13] Heiser J, Soo P. Corrosion of Barrier Materials in Seawater Environments.New York: Long Island, 1995: 23
[14] Fischer K P, Espelid B, Schei B. Corrosion 2001. Houston: NACE, 2001: Paper No.01013
[15] Fischer K P. Corrosion 99. Houston: NACE, 1999: Paper No.361
[16] Chen S, Hatt W, Wolfson S. Corrosion, 2003; 59: 721
[17] Akio K. Corros Sci, 2005; 47: 2361
[18] Mohammed R, Timothy J D. Int J Fatigue, 2008; 30: 2220
[19] Blundy R F, Shreir L L. Corros Sci, 1977; 17: 509
[20] Venkatesan R. PhD Dissertation, Indian Institute of Science, Bangalore, 2000
[21] Beccaria A M, Fiordiponti P, Mattogno G. Corros Sci, 1989; 29: 403
[22] Beccaria A M, Poggi G, Arfelli M, Mattogno G. Corros Sci, 1993; 34: 989
[23] Beccaria A M, Poggi G, Gingaud D, Castello P. Br Corros J, 1994; 29: 65
[24] Beccaria A M, Poggi G. Br Corros J, 1985; 20: 183
[25] Zhu X L, Li L Y, Xu J. Chin J Nonferrous Met, 1998; 8 (suppl 1): 210
(朱小龙, 林乐耘, 徐杰. 中国有色金属学报, 1998; 8(增刊1): 210)
[26] Langenegger E E, Robinson F P A. Corrosion, 1969; 25: 137
[27] Namboodhirl T K G, Chaudhary R S, Prakash B, Agrawal M K. Corros Sci, 1982; 22: 1037
[28] Li Y, Zhu Y L. Corros Prot, 2006; 27: 222
(李勇, 朱应禄. 腐蚀与防护, 2006; 27: 222)
[29] Kear G, Barker B D, Stokes K R, Walsh F C. Electrochim Acta, 2007; 52: 2343
[30] Strandberg H, Johansson L G. J Electrochem Soc, 1998; 145: 1093
[31] Nunea L, Reguera E, Corvo F, Gonzalez E, Vazquez C. Corros Sci, 2005; 47: 461 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|