| 经新型Q-P-T工艺处理后Q235钢的组织与性能 |
| 贾晓帅1,左训伟2,陈乃录1,黄坚1,唐新华 1,戎咏华1 |
| 1.上海交通大学材料科学与工程学院, 上海 200240
2.上海交通大学机械与动力工程学院, 上海 200240 |
|
| MICROSTRUCTURE AND PROPERTIES OF Q235 STEEL TREATED BY NOVEL Q-P-T PROCESS |
| JIA Xiaoshuai1, ZUO Xunwei2, CHEN Nailu1, HUANG Jian1, TANG Xinhua1, RONG Yonghua1 |
| 1. School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240
2. School of Mechanical Engineering, Shanghai Jiao Tong University, Shanghai 200240 |
引用本文:
贾晓帅,左训伟,陈乃录,黄坚,唐新华,戎咏华. 经新型Q-P-T工艺处理后Q235钢的组织与性能[J]. 金属学报, 2013, 49(1): 35-42.
JIA Xiaoshuai,
ZUO Xunwei,
CHEN Nailu,
HUANG Jian,
TANG Xinhua,
RONG Yonghua.
MICROSTRUCTURE AND PROPERTIES OF Q235 STEEL TREATED BY NOVEL Q-P-T PROCESS[J]. Acta Metall Sin, 2013, 49(1): 35-42.
| [1] Xu Z Y. In: Xue Q J ed., The Perspective of Chemical Industry, Metallurgy and Materials,Beijing: Chemical Industry Publishing House, 2007: 403 (徐祖耀. 见: 薛群基主编, 中国工程院化工、冶金与材料工程学部第六届学术会议特邀报告会议论文集,北京: 化学与工业出版社, 2007: 403) [2] Xu Z Y. Heat Treat, 2008; 23(2): 1 (徐祖耀. 热处理, 2008; 23(2): 1) [3] Shang C J, Hu L J, Yang S W, Wang X M, Zhao Y T, He X L. Acta Metall Sin, 2005; 41: 471 (尚成嘉, 胡良均, 杨善武, 王学敏, 赵运堂, 贺信莱. 金属学报, 2005; 41: 471) [4] Liu D S, Cheng B G, Chen Y Y. Acta Metall Sin, 2012; 48: 334 (刘东升, 程丙贵, 陈圆圆. 金属学报, 2012; 48: 334) [5] Qi J J, Yang W Y, Sun Z Q. Acta Metall Sin, 2002; 38: 629 (齐俊杰, 杨王玥, 孙祖庆. 金属学报, 2002; 38: 629) [6] Matlock D K, Speer J G. In: Lee H C ed., The 3rd Int Conf on Advanced Structural Steels, Korea: The Korean Institute of Metals and Materials, 2006: 774 [7] Mileiko S T, Speer J G. J Mater Sci, 1969; 4: 974 [8] Speer J G, Matlock D K, Cooman B C, Schroth J G. Acta Mater, 2003; 51: 2661 [9] Sakuma Y. In: Baker M A ed., Proc Int Conf on Advanced High Strength Sheet Steels for Automotive Applications, Warrendale: Association for Iron-Steel Technology, 2004: 11 [10] Sugimoto K, Kobayshi M, Hashimoto S Y. Metall Trans, 1992; 23: 2085 [11] Speer J G, Assuncao F C R, Matlock D K, Edmonds D V. Mater Res, 2005; 8: 417 [12] Hsu T Y. Mater Sci Forum, 2007; 561: 2283 [13] Wang X D, Zhong N, Rong Y H, Xu Z Y. J Mater Res, 2009; 24: 261 [14] Zhang K, Xu W Z, Guo Z H, Rong Y H, Wang M Q, Dong H. Acta Metall Sin, 2011; 47: 489 (张柯, 许为宗, 郭正洪, 戎咏华, 王毛球, 董瀚. 金属学报, 2011; 47: 489) [15] Zhong N, Wang X D, Wang L, Rong Y H. Mater Sci Eng, 2009; A506: 111 [16] Chen N L, Rong Y H. Chin Pat, 10562008.9, 2010 (陈乃录, 戎咏华. 中国专利, 10562008.9, 2010) [17] Zhou S, Zhang L, Chen N L, Gu J F, Rong Y H. ISIJ Int, 2011; 51: 1688 [18] Liu H P, Lu X W, Jin X J. Mater Des, 2011; 32: 2269 [19] Wang C L. Metal Fracture Analysis. Harbin: Harbin University Press, 1998: 4 (王长利. 金属断口分析. 哈尔滨: 哈尔滨工业大学出版社, 1998: 4) [20] Peng Y, Wang A H, Xiao H J, Tian Z L. Acta Metall Sin, 2012; 48: 1281 (彭云, 王爱华, 肖红军, 田志凌. 金属学报, 2012; 48: 1281) [21] Zhao L, Zhang X D, Chen W Z. Acta Metall Sin, 2005; 41: 392 (赵琳, 张旭东, 陈武柱. 金属学报, 2005; 41: 392) |
|