| 添加Bi对Zr-4合金在400 ℃/10.3 MPa过热蒸汽中耐腐蚀性能的影响 |
| 姚美意1, 2), 邹玲红1, 2), 谢兴飞1, 2), 张金龙1, 2), 彭剑超1, 2), 周邦新1, 2) |
1) 上海大学微结构重点实验室, 上海 200444
2) 上海大学材料研究所, 上海 200072 |
|
| EFFECT OF Bi ADDITION ON THE CORROSION RESISTANCE OF Zr-4 IN SUPERHEATED STEAM AT 400 ℃/10.3 MPa |
| YAO Meiyi1, 2), ZOU Linghong1, 2), XIE Xingfei1, 2), ZHANG Jinlong1, 2), PENG Jianchao1, 2), ZHOU Bangxin1, 2) |
1) Laboratory for Microstructures, Shanghai University, Shanghai 200444
2) Institute of Materials, Shanghai University, Shanghai 200072 |
引用本文:
姚美意 邹玲红 谢兴飞 张金龙 彭剑超 周邦新. 添加Bi对Zr-4合金在400 ℃/10.3 MPa过热蒸汽中耐腐蚀性能的影响[J]. 金属学报, 2012, 48(9): 1097-1102.
,
,
,
,
,
.
EFFECT OF Bi ADDITION ON THE CORROSION RESISTANCE OF Zr-4 IN SUPERHEATED STEAM AT 400 ℃/10.3 MPa[J]. Acta Metall Sin, 2012, 48(9): 1097-1102.
| [1] Sabol G P. In: Rudling P, Kammenzind B eds., Zirconium in the Nuclear Industry: Fourteenth International Symposium, ASTM STP 1467, Stockholm: ASTM International, 2004: 3[2] Sabol G P, Comstock R J, Weiner R A. In: Garde A M, Bradley E R eds., Zirconium in the Nuclear Industry: Tenth International Symposium, ASTM STP 1245, Baltimore, MD: ASTM International, 1994: 724[3] Nikulina A V, Markelov V A, Peregud M M. In: Bradley E R, Sabol G P eds., Zirconium in the Nuclear Industry: Eleventh International Symposium, ASTM STP 1295, Garmisch–Partenkirchen, Germany: ASTM International, 1996: 785[4] Zhao W J, Miao Z, Jiang H M, Yu X W, Li W J, Li C, Zhou B X. J Chin Soc Corros Prot, 2002; 22: 124(赵文金, 苗志, 蒋宏曼, 于晓卫, 李卫军, 李聪, 周邦新. 中国腐蚀与防护学报, 2002; 22: 124)[5] Park J–Y, Yoo S J, Choi B–K, Jeong Y H. J Nucl Mater, 2008; 373: 343[6] Hong H S, Moon J S, Kim S J, Lee K S. J Nucl Mater, 2001; 297: 113[7] Yao M Y, Li S L, Zhang X, Peng J C, Zhou B X, Zhao X S, Shen J Y. Acta Metall Sin, 2011; 47: 865(姚美意, 李士炉, 张欣, 彭剑超, 周邦新, 赵旭山, 沈剑韵. 金属学报, 2011; 47: 865)[8] Li S L, Yao M Y, Zhang X, Geng J Q, Peng J C, Zhou B X. Acta Metall Sin, 2011; 47: 163(李士炉, 姚美意, 张欣, 耿建桥, 彭剑超, 周邦新. 金属学报, 2011; 47: 163)[9] Li P Z, Li Z K. Rare Met Mater Eng, 1998; 27: 356(李佩志, 李中奎. 稀有金属材料与工程, 1998; 27: 356)[10] Zhou B X, Li Q, Yao M Y, Liu W Q. Nucl Power Eng, 2005; 26(4): 364(周邦新, 李 强, 姚美意, 刘文庆. 核动力工程, 2005; 26(4): 364)[11] Li C, Li P, Zhou B X, Zhao W J, Peng Q, Ying S H, Shen B L. Nucl Power Eng, 2002; 23(4): 20(李聪, 李蓓, 周邦新, 赵文金, 彭 倩, 应诗浩, 沈保罗. 核动力工程, 2002; 23(4): 20)[12] Foster J P, Dougherty J, Burke M G. J Nucl Mater, 1990; 173: 164[13] Charquet D. In: Sabol G P, Moan G D eds., Zirconium in the Nuclear Industry: Twelfth International Symposium, ASTM STP 1354, West Conshohocken: ASTM International, 2000: 3[14] Eucken C M, Finden P T. In: Van Swam L F P, Eucken C M eds., Zirconium in the Nuclear Industry: Eighth International Symposium, ASTM STP 1023, Philadelphia: ASTM International, 1989: 113[15] Takeda K, Anada H. In: Sabol G P, Moan G D eds., Zirconium in the Nuclear Industry: Twelfth International Symposium, ASTM STP 1354, West Conshohocken: ASTM International, 2000: 592[16] Garzarolli F, Broy Y, Busch R A. In: Bradley E R, Sabol G P Eds., Zirconium in the Nuclear Industry: Eleventh International Symposium, ASTM STP 1295, Garmisch– Partenkirchen, Germany: ASTM International, 1996: 850[17] Graham R A, Tosdale J P, Finden P T L F P. In: Van Swam L F P, Eucken C M eds., Zirconium in the Nuclear Industry: Eighth International Symposium, ASTM STP 1023, Philadelphia: ASTM International, 1989: 334[18] Yang W D. Reactor Materials Science. 2nd Ed., Beijing: Atomic Energy Press, 2006: 260(杨文斗. 反应堆材料学. 第二版, 北京: 原子能出版社, 2006: 260)[19] Zhou B X, Li Q, Liu W Q, Yao M Y, Chu Y L. Rare Met Mater Eng, 2006; 35: 1009(周邦新, 李强, 刘文庆, 姚美意, 褚于良. 稀有金属材料与工程, 2006; 35: 1009)[20] Cox B. J Nucl Mater, 1969; 29: 50[21] Zhou B X, Li Q, Yao M Y, Liu W Q, Chu Y L. J ASTM Int, 2008; 5: 360[22] Charquet D, Hanh R, Ortlib E. In: Van Swam L F P, Eucken C M eds., Zirconium in the Nuclear Industry, Eighth International Symposium, ASTM STP 1023, Philadelphia: ASTM International, 1989: 405[23] Yao M Y, Zhou B X, Li Q, Liu W Q, Yu W J, Chu Y L. J Nucl Mater, 2008; 374: 197[24] Shen Y F, Yao M Y, Zhang X, Li Q, Zhou B X, Zhao W J. Acta Metall Sin, 2011; 47: 899(沈月锋, 姚美意, 张 欣, 李强, 周邦新, 赵文金. 金属学报, 2011; 47: 899) |
|