梯度NiCrAlY涂层的1000和1100 ℃氧化行为研究 |
于大千,卢旭阳,马军,姜肃猛,刘山川,宫骏,孙超 |
中国科学院金属研究所金属腐蚀与防护国家重点实验室, 沈阳 110016 |
|
STUDY OF OXIDATION BEHAVIOR OF THE GRADIENT NiCrAlY COATING AT 1000 AND 1100 ℃ |
YU Daqian, LU Xuyang, MA Jun, JIANG Sumeng, LIU Shanchuan, GONG Jun, SUN Chao |
State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
于大千,卢旭阳,马军,姜肃猛,刘山川,宫骏,孙超. 梯度NiCrAlY涂层的1000和1100 ℃氧化行为研究[J]. 金属学报, 2012, 48(6): 759-768.
,
,
,
,
,
,
.
STUDY OF OXIDATION BEHAVIOR OF THE GRADIENT NiCrAlY COATING AT 1000 AND 1100 ℃[J]. Acta Metall Sin, 2012, 48(6): 759-768.
[1] Jeanine T D, Dinesh K G. Surf Coat Technol, 1994; 68--69: 1[2] Goward G W. Surf Coat Technol, 1998; 108--109: 73[3] Czech N, Schmitz F, Stamm W. Mater Manuf Processes, 1995; 10: 1021[4] Brandl W, Grabke H J, Toma D, Kruger J. Surf Coat Technol, 1996; 86--87: 41[5] Nicholls J R, Simms N J, Chan W, Evans H E. Surf Coat Technol,2002; 149: 236[6] Ma J, Jiang S M, Li H Q, Wang W X, Gong J, Sun C. Corros Sci,2011; 53: 1417[7] Tang F, Ajdelsztajn L, Schoenung J M. Oxid Met, 2004; 61: 219[8] Wood J H, Swede S T. Surf Coat Technol, 1993; 61: 1[9] Guo M H, Wang Q M, Gong J, Sun C, Wen L S. Surf Coat Technol,2006; 201: 1302[10] Guo M H, Wang Q M, Gong J, Sun C, Huang R F, Wen L S. Corros Sci, 2006; 48: 2750[11] Peng X, Jiang S M, Duan X H, Gong J, Sun C. Acta Metall Sin,2009; 45: 378 (彭新, 姜肃猛, 段绪海, 宫骏, 孙超. 金属学报. 2009; 45: 378)[12] Wang W X, Jiang S M, Wei G Z, Ma J, Gong J, Sun C. Acta Metall Sin,2011; 47: 578 (王维新, 姜肃猛, 卫广智, 马军, 宫骏, 孙超.金属学报. 2011; 47: 578)[13] Jiang S M, Xu C Z, Li H Q, Ma J, Gong J, Sun C. Corros Sci,2010; 52: 1746[14] Lou H Y, Wang F H. Vacuum, 1992; 43: 757[15] Sun C, Wang Q M, Tang Y J, Guan Q F, Gong J, Wen L S. Acta Metall Sin, 2005; 41: 1167 (孙超, 王启民, 唐永吉, 关庆丰, 宫骏, 闻立时. 金属学报,2005; 41: 1167)[16] Xu C Z, Jiang S M, Ma J, Gong J, Sun C. Acta Metall Sin,2009; 45: 964 (徐朝政, 姜肃猛, 马军, 宫骏, 孙超. 金属学报. 2009; 45: 964)[17] Birks N, Meier G H, Pettit F S. Introduction to the High-Temperature Oxidation of Metals. 2nd ed, Cambridge: Cambridge University Press, 2006: 123[18] Lee E Y, Chartier D M, Biederman R R, Sisson Jr R D. Surf Coat Technol, 1987; 32: 19[19] Doychak J. In: Westbrook J H, Fleischer R L, eds., Intermetallic Compounds, New York: John Wiley & Sons Ltd., 1994: 977[20] Li M S. High Temperature Corrosion of Materials.Beijing: Metallurgical Industry Press, 2001: 183 (李美栓. 金属的高温腐蚀. 北京: 冶金工业出版社, 2001: 183)[21] Hagel W C. Corrosion, 1965; 21: 316[22] Rhysjones T N. Corros Sci, 1989; 29: 623[23] Knotek O, Loffler F, Beele W. Surf Coat Technol, 1993; 61: 6[24] Brandl W, Toma D, Kruger J, Grabke H J, Matthaus G. Surf Coat Technol, 1997; 94: 21[25] Rhys--Jones T N. Corros Sci, 1989; 29: 623[26] Morral J E, Thompson M S. Surf Coat Technol, 1990; 43-44: 371[27] Knotek O, Lugscheider E, Lofffler F, Beele W. Surf Coat Technol, 1993; 61: 6[28] Birks N, Meier G H, Pettit F S. Introduction to the High-Temperature Oxidation of Metals. 2nd ed., Cambridge: Cambridge University Press, 2006: 133 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|