| 富Cu团簇的析出对RPV模拟钢韧-脆转变温度的影响 |
| 徐刚1,蔡琳玲1,冯柳1,周邦新1,2,王均安2,张海生3 |
1. 上海大学材料研究所, 上海 200072
2. 上海大学微结构重点实验室, 上海 200444
3. 中国核动力研究设计院核燃料及材料国家重点实验室, 成都 610041 |
|
| EFFECT OF THE PRECIPITATION OF Cu-RICH CLUSTERS ON THE DBTT OF RPV SIMULATED STEEL |
| XU Gang1, CAI Linling1, FENG Liu1, ZHOU Bangxin1,2,WANG Jun'an1,2,ZHANG Haisheng3
|
1. Institute of Materials, Shanghai University, Shanghai 200072
2. Laboratory for Microstructures, Shanghai University, Shanghai 200444
3. National Key Laboratory for Nuclear Fuel and Materials, Nuclear Power Institute of China, Chengdu 610041 |
引用本文:
徐刚,蔡琳玲,冯柳,周邦新,王均安,张海生. 富Cu团簇的析出对RPV模拟钢韧-脆转变温度的影响[J]. 金属学报, 2012, 48(6): 753-758.
,
,
,
,
,
.
EFFECT OF THE PRECIPITATION OF Cu-RICH CLUSTERS ON THE DBTT OF RPV SIMULATED STEEL[J]. Acta Metall Sin, 2012, 48(6): 753-758.
| [1] Toyama T, Nagai Y, Tang Z, Hasegawa M, Almazouzi A, van Walle E,Gerard R. Acta Mater, 2007; 55: 6852[2] Auger P, Pareige P, Welzel S, van Duysen J C. J Nucl Mater,2000; 280: 331[3] Miller M K, Russell K F, Sokolov M A, Nanstad R K. J Nucl Mater,2007; 361: 248[4] Miller M K, Russell K F, Sokolov M A, Nanstad R K. J Nucl Mater,2003; 320: 177[5] Miller M K, Nanstad P K, Sokolov M A, Russell K F. J Nucl Mater,2006; 351: 216[6] Phythian W J, English C A. J Nucl Mater, 1993; 205: 162[7] Carter R G, Soneda N, Dohi K, Hyde J M, English C A, Server W L. J Nucl Mater, 2001; 298: 211[8] Miller M K, Chernobaeva A A, Shtrombakh Y I, Russell K F, Nanstad R K,Erak D Y, Zabusov O O. J Nucl Mater, 2009; 385: 615[9] Miller M K, Russell K F. J Nucl Mater, 2007; 371: 145[10] Hornbogen E, Glenn, R C. Trans Metall Soc AIME, 1960; 218: 1064[11] Zhang R Q, Hong X F, Peng Q. Nucl Power Eng, 2010; 31(1): 4 (张瑞谦, 洪晓峰, 彭倩. 核动力工程. 2010; 31(1): 4)[12] Goodman S R, Brenners S S, Low J R. Metall Trans,1973; 4: 2363[13] Pizzini S, Roberts K J, Phythian W J, English C A, Greaves G N. Philos Mag Lett, 1990; 61: 223[14] Othen P J, Jenkins M L, Smith G D W, Phythian W J. Philos Mag Lett,1991; 64: 383[15] Speich G R, Oriani R A. Trans Metall Soc AIME, 1965; 233: 623[16] Othen P J, Jenkins M L, Smith G D W. Philos Mag, 1994; A70: 1[17] Styman P D, Hyde J M, Wilford K, Morley A, Smith G D W.Prog Nucl Energ, 2011, doi:10.1016/j.pnucene.2011.10.010[18] Chu D F, Xu G, Wang W, Peng J C, Wang J A, Zhou B X. Acta Metall Sin, 2011; 47: 269 (楚大锋, 徐刚, 王伟, 彭剑超, 王均安, 周邦新. 金属学报,2011; 47: 269)[19] Xu G, Cai L L, Feng L, Zhou B X, Wang W, Peng J C. Acta Metall Sin,2011; 47: 906 (徐刚, 蔡琳玲, 冯柳, 周邦新, 王伟, 彭剑超. 金属学报,2011; 47: 906)[20] Miller M K. Atom Probe Tomography: Analysis at the Atomic Level.New York: Kliwer Academic/Plenum Publishers, 2000: 25[21] Yong Q L. Secondary Phase in Steel. Beijing: Metallurgical Industry Press, 2006: 127 (雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 127)[22] Xu G, Cai L L, Feng L, Zhou B X, Liu W Q, Wang J A. Acta Metall Sin, 2012; 48: 407 (徐刚, 蔡琳玲, 冯柳, 周邦新, 刘文庆, 王均安. 金属学报,2012; 48: 407)[23] Buswell J T, English C A, Herherington M G, Phythian W J, Smith G D W, Worral G M. In: Steele L E ed., Proc 14th Int Symp Effects of Radiation on Materials, Vol. 2, Andover, Massachusseetts:The American Society for Testing and Materials, 1990: 127[24] Brown L M, Ham R K. In: Kelly A, Nicholson R B, eds., Strengthening Methods in Crystals. London:Applied Science Publishers; 1965: 9[25] Friedel J. Disloctions. London: Pergamon Press; 1964: 1[26] Russell K C, Brown L M. Acta Metall, 1972; 20: 969[27] Harry T, Bacon D J. Acta Mater, 2002; 50: 195[28] Harry T, Bacon D J. Acta Mater, 2002; 50: 209 |
|