| 5052铝合金板材磁脉冲动态拉伸塑性失稳分析 |
| 刘大海1,于海平2,李春峰2 |
1. 南昌航空大学航空制造工程学院, 南昌 330063
2. 哈尔滨工业大学材料科学与工程学院, 哈尔滨 150001 |
|
| PLASTIC INSTABILITY ANALYSIS OF 5052 ALUMINUM SHEETS IN MAGNETIC DYNAMIC TENSION PROCESS |
| LIU Dahai1,YU Haiping2, LI Chunfeng2 |
1.School of Aeronautical Manufacturing Engineering, Nanchang Hangkong University, Nanchang 330063
2.School of Materials Science and Engineering, Harbin Institute of Technology,Harbin 150001 |
引用本文:
刘大海,于海平,李春峰. 5052铝合金板材磁脉冲动态拉伸塑性失稳分析[J]. 金属学报, 2012, 48(5): 519-525.
,
,
.
PLASTIC INSTABILITY ANALYSIS OF 5052 ALUMINUM SHEETS IN MAGNETIC DYNAMIC TENSION PROCESS[J]. Acta Metall Sin, 2012, 48(5): 519-525.
| [1] Li C F. High Energy Rate Forming. Beijing: National Defense Industry Press, 2001: 1 (李春峰. 高能率成形技术. 北京: 国防工业出版社, 2001: 1)[2] Psyk V, Risch D, Kinsey B L, Tekkaya A E, Kleiner M. J Mater Process Technol, 2011; 5: 787[3] Vohnout V J. PhD Thesis, Ohio State University, Columbus, 1998[4] Balanethiram V S, Daehn G S. Scr Metall, 1992; 27: 1783[5] Balanethiram V S, Daehn G S. Scr Metall, 1994; 30: 515[6] Balanethiram V S, Hu X Y, Daehn G S. J Mater Process Technol,1994; 45: 595[7] Hu X Y, Wagoner R H, Daehn G S, Ghosh S. Metall Trans,1994; 25A: 2723[8] Hu X Y, Daehn G S. Acta Mater, 1996; 44: 1021[9] Oliveira D A, Worswick M J. J Phys IV France, 2003; 110: 293[10] Oliveira D A, Worswick M J, Finn M, Newman D. J Mater Process Technol, 2005; 170: 350[11] Imbert J M, Winkler S L, Worswick M J, Oliveira D A. J Eng Mater Technol, 2005; 27: 127[12] Seth M. PhD Thesis, Ohio State University, Columbus, 2006[13] Thomas J D, Seth M, Daehn G S, Bradley J R, Triantafyllidis N. Acta Mater, 2007; 55: 2863[14] Regazzoni G, Kocks U F, Follansbee P S. Acta Mater, 1987; 35: 2865[15] Follansbee P S, Kocks U F. Acta Mater, 1988; 36: 81[16] Gorham D A. J De Phys III, 1991; 1: 411[17] Dioh N N, Leevers P S, Williams J G. Polymer, 1993; 34: 4230[18] Meyers M A. Dynamic Behavior of Materials. New York: Wiley, 1994[19] Golovashchenko S F. J Mater Eng Perform, 2007; 16: 314[20] Hecker S S. J Eng Mater Technol, 1975; 97H: 66[21] Blazynsk T Z, translated by Li F Q, Wu B Q. Explosive Welding,Forming and Compaction. Beijing: China Machine Press, 1983: 76 (Blazynsk T Z著, 李富勤, 吴柏青译. 爆炸焊接、成形与压制.北京: 机械工业出版社, 1983: 76) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|