| TiNi合金激光焊接接头形状恢复温度的研究 |
| 杨成功1,单际国1, 2,任家烈1 |
1. 清华大学机械工程系, 北京 100084
2. 清华大学先进成形制造教育部重点实验室, 北京 100084 |
|
| STUDY ON SHAPE RECOVERY TEMPERATURE OF TiNi ALLOY LASER WELD JOINT |
| YANG Chenggong1, SHAN Jiguo1,2, REN Jialie1 |
1. Department of Mechanical Engineering, Tsinghua University, Beijing 100084
2. Key Laboratory for Advanced Materials Processing Technology, Ministry of Education, Tsinghua University, Beijing 100084 |
引用本文:
杨成功,单际国,任家烈. TiNi合金激光焊接接头形状恢复温度的研究[J]. 金属学报, 2012, 48(5): 513-518.
,
,
.
STUDY ON SHAPE RECOVERY TEMPERATURE OF TiNi ALLOY LASER WELD JOINT[J]. Acta Metall Sin, 2012, 48(5): 513-518.
| [1] Zhao L C, Cai W, Zheng Y F. Shape Memory Effect and Superelasticity in Alloys. Beijing: National Defense Industry Press, 2002: 5 (赵连成, 蔡伟, 郑玉峰. 合金的形状记忆效应和超弹性.北京: 国防工业出版社, 2002: 5)[2] Xu Z Y. Shape Memory Materials. Shanghai: Shanghai Jiao Tong University Press, 2002: 18 (徐祖耀. 形状记忆材料. 上海: 上海交通大学出版社, 2002: 18)[3] Funakubo H, translate by Qian D F. Shape Memory Alloys.Beijing: China Machine Press, 1984: 85 (Funakubo H 著, 千东范 译. 形状记忆合金. 北京: 机械工业出版社, 1984: 85)[4] Otsuka K, Mayman C M. Shape Memory Materials. Cambridge:Cambridge University Press, 1998: 49[5] Yang J, Wu Y H. Shape Memory Alloys and Their Applications.Hefei: Chinese Science and Technology University Press, 1993: 36 (杨杰, 吴月华. 形状记忆合金及其应用. 合肥: 中国科学技术大学出版社,1993: 36)[6] Ren J L, Wu A P. Joining of Advanced Materials. Beijing:China Machine Press, 2000: 335 (任家烈, 吴爱萍. 先进材料的连接. 北京: 机械工业出版社, 2000: 335)[7] Ikai A, Kimura K, Tobushi H. J Intell Mater Syst Struct,1996; 7: 646[8] Tuissi A, Besseghini S, Ranucci T, Squatrito F, Pozzi M. Mater Sci Eng, 1999; A273-275: 813[9] Hsu Y T, Wang Y R, Chen C. Metall Mater Trans, 2001; 32A: 569[10] Falvo A, Furgiuele F M, Maletta C. Mater Sci Eng, 2005; A412: 235[11] Xu Y L, Cheng Z F, Fan X L, Chu C L, Wang S D. Trans Chin Weld Inst, 2006; 27: 26 (徐越兰, 成志富, 范晓龙, 储成林, 王世栋. 焊接学报, 2006; 27: 26)[12] Falvo A, Furgiuele F M, Maletta C. Mater Sci Eng,2008; A481-482: 647[13] Barcellona A, Fratini L, Palmeri D, Maletta C, Brandizzi M. Int J Mater Form, 2010; 3: 1047[14] Yang C G, Shan J G, Wen P, Ren J L. Acta Metall Sin,2011; 47: 1277 (杨成功, 单际国, 温鹏, 任家烈. 金属学报, 2011, 47: 1277)[15] Xie C Y, Zhao L C, Lei T Q. Acta Aeronaut Astronaut Sin,1991; 12: A395 (谢超英, 赵连成, 雷廷权. 航空学报, 1991; 12: A395)[16] Xie C Y, Zhao L C, Lei T Q. Met Sci Technol, 1990; 9: 118 (谢超英, 赵连成, 雷廷权. 金属科学与工艺, 1990; 9: 118)[17] Michutta J, Somsen C, Yawny A, Dlouhy A, Eggeler G. Acta Mater,2006; 54: 3525[18] Fan G, Chen W, Yang S, Zhu J, Ren X, Otsuka K. Acta Mater,2004; 52: 4351[19] Huang Y S, Lin G M, Lai Q L. Chin J Nonferrous Met, 1993; 3: 57 (黄元士, 林光明, 赖奇略. 中国有色金属学报, 1993; 3: 57) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|