Zr-Sn-Nb新型锆合金板材加工过程中不均匀组织与织构演变 |
陈建伟1, 栾佰峰1, 柴林江1, 余泓冰1, 刘庆1,周军2, 李中奎2 |
1.重庆大学材料科学与工程学院, 重庆 400044
2.西北有色金属研究院, 西安 710016 |
|
HETEROGENEOUS MICROSTRUCTURE AND TEXTURE EVOLUTION DURING FABRICATION OF Zr-Sn-Nb ZIRCONIUM ALLOY SHEETS |
CHEN Jianwei1, LUAN Baifeng1, CHAI Linjiang1, YU Hongbing1, LIU Qing1,ZHOU Jun2, LI Zhongkui2 |
1.College of Materials Science and Engineering, Chongqing University, Chongqing 400044
2.Northwest Institute for Nonferrous Metal Research, Xi'an 710016 |
引用本文:
陈建伟, 栾佰峰, 柴林江, 余泓冰, 刘庆,周军, 李中奎. Zr-Sn-Nb新型锆合金板材加工过程中不均匀组织与织构演变[J]. 金属学报, 2012, 48(4): 393-400.
,
,
,
,
,
,
.
HETEROGENEOUS MICROSTRUCTURE AND TEXTURE EVOLUTION DURING FABRICATION OF Zr-Sn-Nb ZIRCONIUM ALLOY SHEETS[J]. Acta Metall Sin, 2012, 48(4): 393-400.
[1] Srivastava D, Dey G K, Banerjee S. Metall Mater Trans,1995; A26: 2707
[2] Bickel G A, Griffiths M. J Nucl Mater, 2008; 383: 9
[3] Krishna K V M, Sahoo S K, Samajdar I, Neogy S, Tewari R,Srivastava D, Dey G K, Das G H, Saibaba N, Banarjee S. J Nucl Mater,2008; 383: 78
[4] Vaibhaw K, Rao S V R, Jha S K, Saibaba N, Jayaraj R N. J Nucl Mater, 2008; 383: 71
[5] Kumar M K, Vanitha C, Samajdar I, Dey G K, Tewari R, Srivastava D,Banerjee S. J Nucl Mater, 2004; 335: 48
[6] Tewari R, Srivastava D, Dey G K, Chakravarty J K, Banerjee S. J Nucl Mater, 2008; 383: 153
[7] Li Z K, Zhou L, Zhang J J, Wang W S, Jin Z H. Rare Met Mater Eng, 2004; 33: 1362
(李中奎, 周廉, 张建军, 王文生, 金志浩. 稀有金属材料与工程, 2004; 33: 1362)
[8] Woo O T, Tangri K. J Nucl Mater, 1979; 79: 82
[9] Jeong Y H, Rheem K S, Choi C S, Kim Y S. J Nucl Sci Technol,1993; 30: 154
[10] Sahoo S K, Hiwarkar V D, Samajdar I, Dey G K, Srivastav D, Tiwari R,Banerjee S. Scr Mater, 2007; 56: 963
[11] Kumar M K, Vanitha C, Samajdar I, Dey G K, Tewari R, Srivastava D,Banerjee S. Mater Sci Technol, 2006; 22: 331
[12] Dewobroto N, Bozzolo N, Barberis P, Wagner F. Mater Sci Forum,2004; 467-470: 453
[13] Zhu K Y, Chaubet D, Bacroix B, Brisset F. Acta Mater,2005; 53: 5131
[14] Zhu K Y, Bacroix B, Chauveau T, Chaubet D, Castelnau O. Metall Mater Trans, 2009; A40: 2423
[15] Bozzolo N, Dewobroto N, Grosdidier T, Barberis P, Wagner F. Mater Sci Forum, 2004; 467-470: 441
[16] Gerspach F, Bozzolo N, Wagner F. Scr Mater, 2009; 60: 203
[17] Hiwarkar V D, Sahoo SK, Samajdar I, Satpathy A, Krishna K V M, Dey G K, Srivastav D, Tewari R, Banarjee S. J Nucl Mater, 2011; 412: 287
[18] Guo X C, Luan B F, Chen J W, Zhou J, Zhang X Y, Li Z K, Liu Q. Rare Met Mater Eng, 2011; 40: 813
(过锡川, 栾佰峰, 陈建伟, 周军, 张喜燕, 李中奎, 刘庆.稀有金属材料与工程, 2011; 40: 813)
[19] Jung Y I, Lee M H, Kim H G, Park J Y, Jeong Y H. J Alloys Compd, 2009; 479: 423
[20] Kaschner G C, Gray G. Metall Mater Trans, 2000; A31: 1997
[21] McCabe R J, Proust G, Cerreta E K, Misra A. Int J Plast,2009; 25: 454
[22] Francillette H, Bacroix B, Gasperini M, Bechade J L. Acta Mater,1998; 46: 4131
[23] Castelnau O, Francillette H, Bacroix B, Lebensohn R A. J Nucl Mater, 2001; 297: 14
[24] Akhtar A. J Nucl Mater, 1973; 47: 79
[25] Biget M P, Saada G. J Phys III France, 1995; 5: 1833
[26] Yoo M H, Morris J R, Ho K M, Agnew S R. Metall Mater Trans,2002; A33: 813
[27] Akhtar A. Metall Mater Trans, 1975; A6: 1217
[28] Humphreys F J, Ferry M G. Acta Mater, 1996; 44: 2717
[29] Engler O, Hirsch J, Lucke K. Acta Metall Mater,1995; 43: 121
[30] Higginson R L, Aindow M, Bate P S. Mater Sci Eng,1997; A225: 9
[31] Benum S, Nes E. Acta Mater, 1997; 45: 4593
[32] Ibe G, Lucke K. in: Margolin H ed., Recrystallization,Grain Growth and Textures, Ohio, Metals Park: ASM, 1966: 434
[33] Wagner F, Bozzolo N, Van Landuyt O, Grosdidier T. Acta Mater,2002; 50: 1245 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|