| 高结晶度CrN纳米粒子掺杂的DLC薄膜的显微结构及力学性能 |
| 吴忠振, 田修波, 程思达, 巩春志, 杨士勤 |
| 哈尔滨工业大学先进焊接与连接国家重点实验室, 哈尔滨 150001 |
|
| MICROSTRUCTURE AND MECHANICAL PROPERTIES OF DLC FILMS DOPED WITH HIGH CRYSTALLINITY CrN NANOPARTICLES |
| WU Zhongzhen, TIAN Xiubo, CHENG Sida, GONG Chunzhi, YANG Shiqin |
| State Key Lab of Advanced Welding and Joining, Harbin Institute of Technology, Harbin 150001 |
引用本文:
吴忠振 田修波 程思达 巩春志 杨士勤. 高结晶度CrN纳米粒子掺杂的DLC薄膜的显微结构及力学性能[J]. 金属学报, 2012, 48(3): 283-288.
,
,
,
,
.
MICROSTRUCTURE AND MECHANICAL PROPERTIES OF DLC FILMS DOPED WITH HIGH CRYSTALLINITY CrN NANOPARTICLES[J]. Acta Metall Sin, 2012, 48(3): 283-288.
| [1] Liang F, Yan X J. Acta Phys Sin, 1999; 48: 1095(梁风, 严学俭. 物理学报, 1999; 48: 1095)[2] Grill A. Diamond Relat Mater, 1999; 8: 428[3] Chen G H, Yan S G, Zhang F Q. Acta Phys Sin, 1992; 41: 500(陈光华, 阎少光, 张仿清. 物理学报, 1992; 41: 500)[4] Schwarz C, Heeg J, Rosenberg M, Wienecke M. Diamond Relat Mater, 2008; 17: 1685[5] Takeno T, Hoshi Y, Miki H, Takagi T. Diamond Relat Mater, 2008; 17: 1669[6] Gu K M, Tang J N, Li J Q, Yang Q P. J Shenzhen Univ Sci Eng, 2007; 24: 159(谷坤明, 汤皎宁, 李均钦, 杨钦鹏. 深圳大学学报理工版, 2007; 24: 159)[7] Nie C Y, Zhang B Y, Xie H M. Acta Metall Sin, 2007; 43: 1207(聂朝胤, 张碧云, 谢红梅. 金属学报, 2007; 43: 1207)[8] Veprek S, Argon A S. Surf Coat Technol, 2001; 146–147: 175[9] Mourae Silva C W, Branco J R T, Cavaleiro A. Thin Solid Films, 2006; 515: 1063[10] Baba K, Hatada R, Tanaka Y. Surf Coat Technol, 2007; 19–20: 8362[11] Tian X B, Wu Z Z, Gong C Z, Yang S Q. Chin Pat, 201010213894.4, 2010(田修波, 吴忠振, 巩春志, 杨士勤. 中国专利, 201010213894.4, 2010)[12] Kouznetsov V, Mac´ak K, Schneider J M, Helmersson U, Petrov I. Surf Coat Technol, 1999; 122: 290[13] Helmersson U, Lattemann M, Bohlmark J, Ehiasarian A P, Gudmundsson J T. Thin Solid Films, 2006; 513: 1[14] Wu Z Z, Tian X B, Shi J W, Yang S Q, Chu P K. Rev Sci Inst, 2011; 82: 033511[15] Wu Z Z, Tian X B, Wang Z M, Gong C Z, Yang S Q. Chin J Vac Sci Technol, 2011; 31: 1(吴忠振, 田修波, 王泽明, 巩春志, 杨士勤. 真空科学与技术学报, 2011; 31: 1)[16] Li G, Xia L F, Ma X X, Sun Y, Zhan Z J. Acta Metall Sin (Eng Lett), 1999; 12: 551[17] Ji H B, Xia L F, Ma X X, Sun Y, Sun M R. Acta Metall Sin (Eng Lett), 2000; 13: 967[18] Wu Z Z. Master Dissertation, Harbin Institute of technology, 2008(吴忠振. 哈尔滨工业大学硕士学位论文, 2008)[19] Tian X B, Wu Z Z, Shi J W, Li X P, Gong C Z, Yang S Q. Vacuum, 2010; 47: 44(田修波, 吴忠振, 石经伟, 李希平, 巩春志, 杨士勤. 真空, 2010; 47: 44)[20] Anders A. Surf Coat Technol, 1997; 93: 158[21] Martin P J, Bendavid A, Cairney J M, Hoffman M. Surf Coat Technol, 2005; 200: 2228[22] Ma D Y, Ma S L, Xu K W. Acta Metall Sin, 2004; 40: 1037(马大衍, 马胜利, 徐可为. 金属学报, 2004; 40: 1037)[23] Guo Y, Xu B, Wu G Z, Ma S L, Xu K W. Acta Metall Sin, 2007; 43: 159(郭岩, 徐 彬, 吴贵智, 马胜利, 徐可为. 金属学报, 2007; 43: 159)[24] Alami J, Sarakinos K, Uslu F, Wuttig M. J Phys D: Appl Phys, 2009; 42: 015304[25] Vyas A, Shen Y G, Zhou Z F, Li K Y. Compos Sci Technol, 2008; 68: 2922[26] Shi Y, Long S, Liang F. Appl Surf Sci, 2008; 254: 5861[27] Yang Y Y, Peng Z J, Fu Z Q, Wu S D, Chen X C, Wang C B. Acta Metall Sin, 2010; 46: 34(杨义勇, 彭志坚, 付志强, 邬苏东, 陈新春, 王成彪. 金属学报. 2010; 46: 34)[28] Yang W J, Choa Y–H, Sekino T, Shim K B, Niihara K, Auh K H. Thin Solid Films, 2003; 434: 49[29] Jiang B L, Hu P F, Li H T. Trans Mater Heat Treat, 2010; 31: 134(蒋百灵, 胡鹏飞, 李洪涛. 材料热处理学报. 2010; 31: 134)[30] Niu S C, Yu Z M, Dai M J, Lin S S, Hou H J, Li H W. China Surf Eng, 2007; 20: 34(牛仕超, 余志明, 代明江, 林松盛, 候惠君, 李洪武. 中国表面工程. 2007; 20: 34)[31] Veprek S, Niederhofer A, Moto K, Bolom T, Mannling H–D, Nesladek P, Dollinger G, Bergmaier A. Surf Coat Technol, 2000; 133–134: 152[32] Robertson J. Mater Sci Eng, 2002; R37: 129 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|