| 海藻希瓦氏菌对Zn-Al-Cd牺牲阳极的腐蚀性能影响 |
| 张杰1,宋秀霞1,2,栾鑫1,3,孙彩霞1,4,段继周1,侯保荣1 |
1. 中国科学院海洋研究所, 青岛 266071
2. 上海海洋大学水产与生命学院, 上海 201306
3. 中国海洋大学海洋生命学院, 青岛 266100
4. 烟台大学化学化工学院, 烟台 264005 |
|
| EFFECTS OF SHEWANELLA ALGAE ON CORROSION OF Zn–Al–Cd ANODE |
| ZHANG Jie 1, SONG Xiuxia 1,2, LUAN Xin 1,3, SUN Caixia 1,4, DUAN Jizhou 1,HOU Baorong 1 |
1. Institute of Oceanology, Chinese Academy of Sciences, Qingdao 266071
2. College of Fisheries and Life Science, Shanghai Ocean University, Shanghai 201306
3. College of Marine Life Sciences, Ocean University of China, Qingdao 266100
4. Chemistry and Chemical Engineering College, Yantai University, Yantai 264005 |
引用本文:
张杰 宋秀霞 栾鑫 孙彩霞 段继周 侯保荣. 海藻希瓦氏菌对Zn-Al-Cd牺牲阳极的腐蚀性能影响[J]. 金属学报, 2012, 48(12): 1495-1502.
ZHANG Jie SONG Xiuxia LUAN Xin SUN Caixia DUAN Jizhou HOU Baorong.
EFFECTS OF SHEWANELLA ALGAE ON CORROSION OF Zn–Al–Cd ANODE[J]. Acta Metall Sin, 2012, 48(12): 1495-1502.
| [1] Wu J Y, Chai K, Xiao W L, Yang Y H, Han E H. Acta Metall Sin, 2010; 46: 755(吴进怡, 柴 柯, 肖伟龙, 杨雨辉, 韩恩厚. 金属学报, 2010; 46: 755)[2] Dumas C, Basseguy R, Bergel A. Electrochim Acta, 2008; 53: 5235[3] Mansfeld F. Electrochim Acta, 2007; 52: 7670[4] MacDonell M T, Colwell R R. Int J Syst Evol Microbiol, 1985; (6): 171[5] Manohar A K, Bretschger O, Nealson K H, Mansfeld F. Bioelectrochem, 2008; 72: 149[6] Manohar A K, Mansfeld F. Electrochim Acta, 2009; 54: 1664[7] Mohan S V, Raghavulu S V, Sarma P N. Biosens Bioelectron, 2008; 24: 41[8] Lee A K, Newman D K. Appl Microbiol Biotechnol, 2003; 63(1): 134[9] Wang H B, Hu C, Hu X X, Yang M, Qu J H. Water Res, 2012; 46: 1070[10] Dubiel M, Hsu C H, Chien C C, Mansfeld F, Newman D K. Appl Environ Microbiol, 2002; 68: 1440[11] Herrera L K, Videla H A. Int Biodeterior Biodegrad, 2009; 63: 891[12] Lee A K, Buehler M G, Newman D K. Corros Sci, 2006; 48: 165[13] Kus E, Nealson K, Mansfeld F. Corros Sci, 2007; 49: 3421[14] Nagiub A, Mansfeld F. Electrochim Acta, 2002; 47: 2319[15] Nozue H, Hayashi T, Hashimoto Y, Ezaki T, Hamasaki K, Owada K. Int J Syst Bacteriol, 1992; 42: 628[16] Guha H, Jayachandran K, Maurrasse F. Environ Pollut, 2001; 115: 209[17] Shin H Y, Singhal N, Park J W. Chemosphere, 2007; 68: 1129[18] Long P, Li Q F. Corros Sci Prot Technol, 2007; 19: 235(龙萍, 李庆芬. 腐蚀科学与防护技术, 2007; 19: 235)[19] Rousseau C, Baraud F, Leleyter L, Gil O. J Hazard Mater, 2009; 167: 953[20] Mottin E, Caplat C, Latire T, Mottier A, Mahaut M L, Costil K, Barillier D, Lebel J M, Serpentini A. Mar Pollut Bull, 2012; http://dx.doi.org/10.1016/j.marpolbul.2012.06.017[21] Wagner P, Little B, Hart K, Ray R, Thomas D, Trzaskoma–Paulette P, Lucas K. Int Biodeterior Biodegrad, 1996; 37: 151[22] Zhang J, Liu F L, Li W H, Duan J Z, Hou B R. Acta Metall Sin, 2010; 46: 1250(张杰, 刘奉令, 李伟华, 段继周, 侯保荣. 金属学报, 2010; 46: 1250)[23] Liu J H, Liu F, Li S M. Corros Sci Prot Technol, 2001; 13: 85(刘建华, 刘芳, 李松梅. 腐蚀科学与防护技术, 2001; 13: 85)[24] Mansfeld F. Electrochim Acta, 2007; 52: 7670 [25] Liu J H, Liang X, Li S M. J Chin Rare Earth Soc, 2006; 24: 81(刘建华, 梁馨, 李松梅. 中国稀土学报, 2006; 24: 81)[26] Wan Y, Zhang D, Liu H Q, Li Y J, Hou B R. Electrochim Acta, 2010; 55: 1528[27] Liu G Z, Qian J H, Ma Y, Wu J H. J Electrochem, 2002; 8: 191(刘光洲, 钱建华, 马 焱, 吴建华. 电化学, 2002; 8: 191)[28] Liu J, Yan Y G, Chen G Z, Liu G Z, Li Q F. J Electrochem, 2006; 12: 93 (林晶, 阎永贵, 陈光章, 刘光州, 李庆芬. 电化学, 2006; 12: 93)[29] Long P, Yang S W, Luo Z H. Appl Sci Technol, 2003; 30(7): 1(龙萍, 杨世伟, 罗兆红. 应用科技, 2003; 30(7): 1) |
|