| Zr-0.7Sn-0.35Nb-0.3Fe-xGe合金在高温高压LiOH 水溶液中耐腐蚀性能的研究 |
| 谢兴飞1,2,张金龙1,2,朱莉1,2,姚美意1,2,周邦新1,2,彭剑超1,2 |
1. 上海大学微结构重点实验室, 上海 200444
2. 上海大学材料研究所, 上海 200072 |
|
| STUDY ON THE CORROSION RESISTANCE OF Zr–0.7Sn–0.35Nb–0.3Fe–xGe ALLOY IN LITHIATEDWATER AT HIGH TEMPERATURE UNDER HIGH PRESSURE |
| XIE Xingfei 1,2, ZHANG Jinlong 1,2, ZHU Li 1,2, YAO Meiyi 1,2, ZHOU Bangxin 1,2, PENG Jianchao 1,2 |
1. Laboratory for Microstructures, Shanghai University, Shanghai 200444
2. Institute of Materials, Shanghai University, Shanghai 200072 |
引用本文:
谢兴飞 张金龙 朱莉 姚美意 周邦新 彭剑超. Zr-0.7Sn-0.35Nb-0.3Fe-xGe合金在高温高压LiOH 水溶液中耐腐蚀性能的研究[J]. 金属学报, 2012, 48(12): 1487-1494.
XIE Xingfei ZHANG Jinlong ZHU Li YAO Meiyi ZHOU Bangxin PENG Jianchao.
STUDY ON THE CORROSION RESISTANCE OF Zr–0.7Sn–0.35Nb–0.3Fe–xGe ALLOY IN LITHIATEDWATER AT HIGH TEMPERATURE UNDER HIGH PRESSURE[J]. Acta Metall Sin, 2012, 48(12): 1487-1494.
| [1] Liu J Z. Structure Nuclear Materials. Beijing: Chemical Industry Press, 2007: 19(刘建章. 核结构材料. 北京: 化学工业出版社, 2007: 19)[2] Zhao W J, Zhou B X, Miao Z, Peng Q, Jiang Y R, Jiang H M, Pang H. Atom Energ Sci Technol, 2005; 39(suppl):1(赵文金, 周邦新, 苗志, 彭倩, 蒋有荣, 蒋宏曼, 庞华. 原子能科学技术, 2005; 39(增刊): 1)[3] Nikulina A V, Markelov V A. In: Bradley E R, Sabol G P eds., Zirconium in the Nuclear Industry: 11th International Symposium, ASTM STP 1295, GarmischPartenkirchen Germany: ASTM International, 1996: 785[4] Sabol G P, Comstock R J. In: Garde A M, Bradley E R eds., Zirconium in the Nuclear Industry: 10th International Symposium, ASTM STP 1245, Baltimore, MD:ASTM International, 1994: 724[5] Jung Y I, Lee M H, Kim H G, Park J Y, Jeong Y H. J Alloys Compd, 2009; 479: 423[6] Yang W D. Reactor Materials Science. 2nd Ed., Beijing: Atomic Energy Press, 2006: 260(杨文斗. 反应堆材料学. 第二版, 北京: 原子能出版社, 2006: 260)[7] Liu W Q, Zhu X Y, Wang X J, Li Q, Yao M Y, Zhou B X. Atom Energ Sci Technol, 2010; 44: 1477(刘文庆, 朱晓勇, 王晓娇, 李强, 姚美意, 周邦新. 原子能科学技术, 2010; 44: 1477)[8] Kim J M, Jeong Y H, Kim I S. J Nucl Mater, 2000; 280: 235[9] Liu W Q, Li Q, Zhou B X, Yao M Y. Nucl Power Eng, 2003; 24(1): 33(刘文庆, 李强, 周邦新, 姚美意. 核动力工程, 2003; 24(1): 33)[10] Wang J K. Modern Ge Metallurgy. Beijing: Metallurgy Industry Press, 2005: 58(王吉坤. 现代锗冶金. 北京: 冶金工业出版社, 2005: 58)[11] Zhou B X, Li Q, Yao M Y, Liu W Q, Chu Y L. In: Kammenzind B, Limback M eds., Zirconium in the Nuclear Industry: 15th International Symposium, ASTM STP 1505,West Conshohochen: American Society for Testing and Materials, 2009: 360[12] Schaffer M, Schaffer B, Ramasse Q. Ultramicroscopy, 2012; 114: 62[13] Zhou B X, Yao M Y, Li Q, Xia S, Liu W Q, Chu Y L. Rare Met Mater Eng, 2007; 36: 1317(周邦新, 姚美意, 李强, 夏爽, 刘文庆, 褚于良. 稀有金属材料与工程, 2007; 36: 1317)[14] Charquet D, Hahn R, Ortlib E. In: Van Swam L F P, Eucken C M eds., Zircorium in the Nuclear Industry: 8th International Symposium, ASTM STP 1023, Philadelphia:ASTM International, 1989: 405[15] Anada H, Takeda K. In: Sabol G P, Bradley E R eds., Zircorium in the Nuclear Industry: 11th International Symposium, ASTM STP 1295, Ann Arbor: ASTM International,1996: 35[16] Wadman B, Lai Z, Andren H O, Nystrom A L, Rudling P, Pettersson H. In: Garde A M, Bradley E R eds., Zirconium in the Nuclear Industry: 10th International SymposiumASTM STP 1245, Ann Arbor: ASTM International, 1994: 579[17] Zhou B X, Peng J C, Yao M Y, Li Q, Xia S, Du C X, Xu G. In: Limback M, Barb´eris P eds., Zirconium in the Nuclear Industry: 16th International Symposium, ASTMSTP 1529, Bridgeport: ASTM International, 2011: 620[18] Zhang X, Yao M Y, Li S L, Zhou B X. Acta Metall Sin, 2011; 47: 1112(张欣, 姚美意, 李士炉, 周邦新. 金属学报, 2011; 47: 1112)[19] Zhou B X, Li Q, Liu W Q, Yao M Y, Chu Y L. Rare Met Mater Eng, 2006; 35: 1009(周邦新, 李强, 刘文庆, 姚美意, 褚于良. 稀有金属材料与工程, 2006; 35: 1009)[20] Zhou B X, Li Q, Yao M Y, Liu W Q, Chu Y L. Corros Prot, 2009; 30: 589(周邦新, 李强, 姚美意, 刘文庆, 褚于良. 腐蚀与防护, 2009; 30: 589)[21] Li T F. Metal High Temperature Oxidation and Thermal Corrosion. Beijing: Chemical Industry Press, 2003: 51(李铁藩. 金属高温氧化和热处理. 北京: 化学工业出版社, 2003: 51)[22] Yang X L, Zhou B X, Jiang Y R, Li C. Nucl Power Eng, 1994; 15(1): 79(杨晓林, 周邦新, 蒋有荣, 李聪. 核动力工程, 1994; 15(1): 79)[23] Toffolon–Masclet C, Brachet J C, Jago G. J Nucl Mater, 2002; 305: 224[24] Cao X X, Yao M Y, Peng J C, Zhou B X. Acta Metall Sin, 2011; 47: 882(曹潇潇, 姚美意, 彭剑超, 周邦新. 金属学报, 2011; 47: 882)[25] Yilmazbayhan A, Breval E. J Nucl Mater, 2006; 349: 265 |
|