| Si和Y掺杂对(Ti, Al)N涂层结构和性能的影响 |
| 范永中, 张淑娟, 涂金伟, 孙霞, 刘芳, 李明升 |
| 江西科技师范学院江西省材料表面工程重点实验室, 南昌 330013 |
|
| INFLUENCE OF DOPING WITH Si AND Y ON STRUCTURE AND PROPERTIES OF (Ti, Al)N COATING |
| FAN Yongzhong, ZHANG Shujuan, TU Jinwei, SUN Xia, LIU Fang, LI Mingsheng |
| Jiangxi Key Laboratory of Surface Engineering, Jiangxi Science and Technology Normal University, Nanchang 330013 |
引用本文:
范永中 张淑娟 涂金伟 孙霞 刘芳 李明升. Si和Y掺杂对(Ti, Al)N涂层结构和性能的影响[J]. 金属学报, 2012, 48(1): 99-106.
,
,
,
,
,
.
INFLUENCE OF DOPING WITH Si AND Y ON STRUCTURE AND PROPERTIES OF (Ti, Al)N COATING[J]. Acta Metall Sin, 2012, 48(1): 99-106.
| [1] Paldey S, Deevi S C. Mater Sci Eng, 2003; A3: 58[2] Mayrhofer P H, Mitterer C, Hultman L, Clemens H. Prog Mater Sci, 2006; 51: 1032[3] Ma S L, Jie W Q, Xu K W. Chin J Vac Sci Technol, 2002; 22: 438(马胜利, 介万奇, 徐可为. 真空科学与技术学报, 2002; 22: 438)[4] Inoue S, Uchida H, Yoshinaga Y, Koterazawa K. Thin Solid Films, 1997; 300: 171[5] Li M S, Wang F H, Wang T G, Gong J, Sun C, Wen L S. Acta Metall Sin, 2003; 39: 55(李明升, 王福会, 王铁钢, 宫俊, 孙超, 闻立时. 金属学报, 2003; 39: 55)[6] Makino Y. Surf Coat Technol, 2005; 193: 185[7] Pilloud D, Pierson J F, Marco de Lucas M C, Cavaleiro A. Surf Coat Technol, 2008; 202: 2413[8] Veprek S, Reiprich S, Shizi L. Appl Phys Lett, 1995; 66: 2640[9] Vaz F, Rebouta L, Andritschky M, Silva M, Soares J C. Surf Coat Technol, 1998; 98: 912[10] Pfeiler M, Zechner J, Penoy M, Michotte C, Mitterer C, Kathrein M. Surf Coat Technol, 2009; 203: 3104[11] Lembke M I, Lewis D B, M¨unz W D, Titchmarsh J M. Surf Eng, 2001; 17: 153[12] Li M S, Feng C J, Wang F H. Funct Mater (suppl), 2007; (38): 2615(李明升, 冯长杰, 王福会. 功能材料(增刊), 2007; (38): 2615)[13] Mao Y F, Tang W G, Liu J L, Han P G. Tool Eng, 2006; 40: 20(毛延发, 唐为国, 刘金良, 韩培刚. 工具技术, 2006; 40: 20)[14] Jung H G, Kim K Y. Oxid Met, 1998; 49: 403[15] Flink A, Andersson J M, Alling B, Daniel R, Sjolen J, Karlsson L, Hultman L. Thin Solid Films, 2008; 517: 714[16] Carvalho S, Rebouta L, Ribeiro E, Vaz F, Tavares C J, Alves E, Barradas N P, Riviere J P. Vacuum, 2009; 83: 1206[17] Vennemann A, Stock H R, Kohlscheen J, Rambadt S, Erkens G. Surf Coat Technol, 2003; 174–175: 408[18] Wang F Z, Ma W C. Vapor Deposition Applications Technology. Beijing: China Machine Press, 2006: 291(王福贞, 马文存. 气相沉积应用技术. 北京: 机械工业出版社, 2006: 291)[19] Makino Y. Mater Sci Eng, 1995; 2: 67[20] Vaz F, Rebouta L, Andritschky M, Silva M, Soares J C. J Eur Ceram Soc, 1997; 17: 1971[21] Banakh O, Schmid P E, Sanjines R, Levy F. Surf Coat Technol, 2003; 163: 57[22] Chang Y Y, Hsiao C Y. Surf Coat Technol, 2009; 204: 992[23] M¨unz W D. Werkst Korros, 1990; 41: 753[24] Veprek S, Sarott F A, Iqbal Z. Phys Rev, 1987; B36: 3344[25] Veprek S, Maritza G J, Veprek H, Karvankova P, Prochazka J. Thin Solid Films, 2005; 476: 1[26] Raveh A, Zukerman I, Shneck R, Avni R, Fried I. Surf Coat Technol, 2007; 201: 6136[27] Tanaka Y, Ichimiya N, Onishi Y, Yamada Y. Surf Coat Technol, 2001; 146–147: 215[28] Carvalho S, Rebouta L, Cavaleiro A, Rocha L A, Gomes J, Alves E. Thin Solid Films, 2001; 398–399: 391 |
|