X70钢在模拟潮湿存储环境中的点蚀行为 |
刘智勇1,2,董超芳1,贾志军1,李晓刚1 |
1. 北京科技大学腐蚀与防护中心腐蚀与防护教育部重点实验室, 北京 100083
2. 南昌航空大学材料科学与工程学院, 南昌 330063 |
|
PITTING CORROSION OF X70 PIPELINE STEEL IN THE SIMULATED WET STORAGE ENVIRONMENT |
LIU Zhiyong 1,2, DONG Chaofang 1, JIA Zhijun 1, LI Xiaogang 1 |
1. Corrosion and Protection Center University of Science and Technology Beijing, Key Laboratory of Corrosion and Protection of Ministry of Education, Beijing 100083
2. School of Material Science and Technology, Nanchang Hangkong University, Nanchang 330063 |
引用本文:
刘智勇 董超芳 贾志军 李晓刚. X70钢在模拟潮湿存储环境中的点蚀行为[J]. 金属学报, 2011, 47(8): 1009-1016.
,
,
,
.
PITTING CORROSION OF X70 PIPELINE STEEL IN THE SIMULATED WET STORAGE ENVIRONMENT[J]. Acta Metall Sin, 2011, 47(8): 1009-1016.
[1] Li M C, Cheng Y F. Electrochim Acta, 2007; 53: 2831
[2] Manfredi C, Otegui J L. Eng Fail Analy, 2002; 9: 495
[3] Ramanarayanan T A, Smith S N. Corrosion, 1990; 43: 4001
[4] Azevedo C R F. Eng Fail Analy, 2007; 14: 978
[5] Albarran J L, Martinez L, L´opez H F. Scr Mater, 1998; 38: 749
[6] Chattoraj I, Tiwari S B, Ray A K. Corros Sci, 1995; 37: 885
[7] Parkins R N, Blanchard Jr W K, Delanty B S. Corrosion, 1994; 50: 394
[8] Park J J, Pyun S I, Na K H, Kho Y T. Corrosion, 2002; 58: 329
[9] Beavers J A, Harle B A. J OffshMech Arc Eng, 2001; 123: 147
[10] Hardie D, Charles E A, Lopez A H. Corros Sci, 2006; 48: 4378
[11] Gu B, Luo J, Mao X. Corrosion, 1999; 55: 96
[12] Yang Z P. Pipel Tech Equip, 1999; (5): 12
(杨祖佩. 管道技术与设备, 1999; (5): 12)
[13] Liu Z Y, Dong C F, Li X G. Chin J Mech Eng, 2011; 47:62
(刘智勇, 董超芳, 李晓刚. 机械工程学报, 2011; 47: 62)
[14] Van Boven G, Chen W, Rogge R. Acta Mater, 2007; 55: 29
[15] Li L,Wang C, Yuan B Y, Chen S H. Electrochem Communi, 2008; 10: 103
[16] Laycock N J, Newman R C. Corros Sci, 1997; 39: 1771
[17] Frankel G S. J Electrochem Soc, 1998; 145: 2186
[18] Jia Z J, Li X G, Dong C F, Cheng Y F. Eng Fail Analy, 2009; 16: 2342
[19] Li W S, Cui N, Luo J L. Electrochim Acta, 2004; 49: 1663
[20] Pickering H W. Corros Sci, 1989; 29: 325
[21] Nesic S, Postlethwaite J, Olsen S. Corrosion, 1996; 52: 280
[22] Li M C, Lin H C, Cao C N. J Chin Soc Corros Prot, 2000; 20: 111
(李谋成, 林海潮, 曹楚南. 中国腐蚀与防护学报, 2000; 20: 111)
[23] Ernst P, Newman R C. Corros Sci, 2002; 44: 943 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|