| 瞬态热冲击环境下超硬铝合金7A04的力学性能 |
| 吴大方,潘兵,王岳武,赵寿根,杨洪源,黄良 |
| 北京航空航天大学航空科学与工程学院, 北京 100191 |
|
| MECHANICAL PROPERTIES OF SUPER–HIGH STRENGTH Al ALLOY 7A04 AT TRANSIENT HEATING |
| WU Dafang, PAN Bing, WANG Yuewu, ZHAO Shougen, YANG Hongyuan, HUANG Liang |
| School of Aeronautical Science and Engineering, Beijing University of Aeronautics and Astronautics, Beijing, 100191 |
引用本文:
吴大方 潘兵 王岳武 赵寿根 杨洪源 黄良. 瞬态热冲击环境下超硬铝合金7A04的力学性能[J]. 金属学报, 2011, 47(6): 757-762.
,
,
,
,
,
.
MECHANICAL PROPERTIES OF SUPER–HIGH STRENGTH Al ALLOY 7A04 AT TRANSIENT HEATING[J]. Acta Metall Sin, 2011, 47(6): 757-762.
| [1] Kapoor K, Murlidharan K, Sreedharan K M. J Mater Eng Perform, 1995; 4: 610[2] Witkin D, Han B Q, Lavernia E J. J Mater Eng Perform, 2005; 14: 519[3] Taleff E M, Nevland P J, Krajewski P E. Metall Mater Trans, 2001; 32A: 1119[4] Tang Z L, Yan X D, Li J P, Xu X J, Mao B P, Shen J. Chin J Rare Met, 2010; 34: 516(汤振雷, 闫晓东, 李俊鹏, 许晓静, 毛柏平, 沈健. 稀有金属, 2010: 34: 516)[5] Zhang X M, Liu B, Liu Y, Li H Z, Li H J. Chin J Nonferrous Met, 2007; 17: 1561(张新明, 刘波, 刘瑛, 李慧中, 李惠杰. 中国有色金属学报,2007; 17: 1561)[6] Yang Y M, Peng X H, Chen Y Z, Yin Y HChen G. Acta Metall Sin, 2000; 36: 926(杨运民, 彭向和, 陈裕泽, 尹益辉, 陈刚. 金属学报, 2000; 36: 926)[7] Han M B, Liu Z D, Liu Y G. Expl Shock Waves, 1999; 19(1): 20(韩铭宝, 刘宗德, 刘怡光. 爆炸与冲击, 1999; 19(1): 20)[8] Tan Y, Yu Y, Pan X X, Li G D, Zhang F J, Feng J, Zhou D H, Rong L J, Ma L M. Acta Metall Sin, 2002; 38: 684(谭云, 余勇, 潘晓霞, 李光东, 张方举, 丰 杰, 周德惠,戎利建, 马禄铭. 金属学报, 2002; 38: 684)[9] Kaschniz E, Reiter P, McClure J L. Int J Thermophys, 2002; 23: 267[10] Sameshima T, Kaneko Y, Andoh N. Mater Sci Process,2002; 74A: 719[11] CheB, Peng X H, Yang Y M, Wang J. Acta Metall Sin, 2001; 37: 1256(陈斌, 彭向和, 杨运民, 王军. 金属学报, 2001; 37: 1256)[12] Li M, Song Y Q, Cui S, YU X Z, Li Z DChinese J Rare Met, 2007; 31: 420(李明, 宋月清, 崔舜, 于兴哲, 李增德. 稀有金属, 2007; 31: 420)[13] Wu D F, Fang Y P, Zhang M. Aviat Metrol Meas Technol, 2003; 23(1): 9(吴大方, 房元鹏, 张敏. 航空计测技术, 2003; 23(1): 9)[14] Wu D F, Gao Z T, Wang Y H. J Beijing Univ Aeronaut Astronaut, 2000; 28: 682(吴大方, 高镇同, 王永海. 北京航空航天大学学报, 2000; 28: 682)[15] The Editorial Board of China Aeronautical Materials Handbook. China Aeronautical Materials Handbook. 2nd ed. Vol.3. Beijing: Standard Press of China, 2002: 247(《中国航空材料手册》编辑委员会. 中国航空材料手册(第2版). 第三卷. 北京: 中国标准出版社, 2002: 247) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|