| Ar气泡在连铸坯固/液界面处运动行为的物理模拟研究 |
| 金小礼,雷作胜,于湛,张浩斌,邓康,任忠鸣 |
| 上海大学上海市现代冶金与材料制备重点实验室, 上海 200072 |
|
| PHYSICAL SIMULATION OF Ar BUBBLE BEHAVIOR IN THE SOLID/LIQUID INTERFACE OF CONTINUOUS CASTING BILLET |
| JIN Xiaoli, LEI Zuosheng, YU Zhan, ZHANG Haobin, DENG Kang, REN Zhongming |
| Shanghai Key Laboratory of Modern Metallurgy & Materials Processing, Shanghai University, Shanghai 200072 |
引用本文:
金小礼 雷作胜 于湛 张浩斌 邓康 任忠鸣. Ar气泡在连铸坯固/液界面处运动行为的物理模拟研究[J]. 金属学报, 2011, 47(6): 763-768.
,
,
,
,
,
.
PHYSICAL SIMULATION OF Ar BUBBLE BEHAVIOR IN THE SOLID/LIQUID INTERFACE OF CONTINUOUS CASTING BILLET[J]. Acta Metall Sin, 2011, 47(6): 763-768.
| [1] Zhang L, Aoki J, Thomas B G. Metall Mater Trans, 2006; 37B: 361[2] Pfeiler C, Wu M, Ludwig A. Mater Sci Eng, 2005; A413–414: 115[3] Thomas B G, Huang X, Sussman R C. Metall Mater Trans, 1994; 25B: 527[4] Singh V, Dash S K, Sunitha J S, Ajmani S K, Das A K. ISIJ Int, 2006; 46: 210[5] Yu H Q, Zhu M Y. Acta Metall Sin, 2008; 44: 619(于海岐, 朱苗勇. 金属学报, 2008; 44: 619)[6] Yu H Q, Zhu M Y. Acta Metall Sin, 2008; 44: 1141(于海岐, 朱苗勇. 金属学报, 2008; 44: 1141)[7] Yu H X, Zhu G S, Wang X H, Zhang J M, Wang W J. J Univ Sci Technol Beijing, 2003; 25: 215(于会香, 朱国森, 王新华, 张炯明, 王万军. 北京科技大学学报, 2003, 25: 215)[8] Zhang S J, Zhu M Y, Zhang Y L, Zheng G S, Cheng N L, Song J X. Acta Metall Sin, 2006; 42: 1087(张胜军, 朱苗勇, 张永亮, 郑淑国, 程乃良, 宋景欣. 金属学报, 2006; 42: 1087)[9] Cao N, Zhu M Y. Acta Metall Sin, 2008; 44: 79(曹 娜, 朱苗勇. 金属学报, 2008; 44: 79)[10] Cao N, Zhu M Y. Acta Metall Sin, 2008; 44: 626(曹娜, 朱苗勇. 金属学报, 2008; 44: 626)[11] Feng W, Zhu C Y, Yu T J, Zhang H L, Liu C J, Jiang M F. Contin cast, 2007; (4): 4(冯巍, 朱传运, 余挺进, 张红令, 刘承军, 姜茂发. 连铸, 2007; (4): 4)[12] Lei H, Zhu M Y, He J C. Int J Cast Met Res, 2007; 20: 98[13] Esaka H, Kuroda Y, Shinozuka K, Tamura M. ISIJ Int, 2004; 44: 682[14] Chen Z H, Wang E G, Zhang X W, He J C. Acta Metall Sin, 2007; 43: 422(陈芝会, 王恩刚, 张兴武, 赫冀成. 金属学报, 2007; 43: 422)[15] Lei Z S, Zhang H B, Ren Z M, Deng K. J Iron Steel Res Int, 2008; 15(Suppl. 1): 538[16] Yu Z, Zhang Z Q, Ren Z M, Lei Z S, Deng K. Acta Metall Sin, 2010; 46: 1275(于湛, 张振强, 任忠鸣, 雷作胜, 邓康. 金属学报, 2010; 46: 1275) |
|