| 热压烧结温度对SiC颗粒增强铝基复合材料微观组织及力学性能的影响 |
| 金鹏,肖伯律,王全兆,马宗义,刘越,李曙 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016 |
|
| EFFECT OF HOT PRESSING TEMPERATURE ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF SiC PARTICLE REINFORCED ALUMINUM
MATRIX COMPOSITES |
| JIN Peng, XIAO Bol¨u, WANG Quanzhao, MA Zongyi, LIU Yue, LI Shu |
| Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
金鹏 肖伯律 王全兆 马宗义 刘越 李曙. 热压烧结温度对SiC颗粒增强铝基复合材料微观组织及力学性能的影响[J]. 金属学报, 2011, 47(3): 298-304.
,
,
,
,
,
.
EFFECT OF HOT PRESSING TEMPERATURE ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF SiC PARTICLE REINFORCED ALUMINUM
MATRIX COMPOSITES[J]. Acta Metall Sin, 2011, 47(3): 298-304.
| [1] Ouyang Q B, Li R X, Wang W L, Zhang G D, Zhang D. Mater Sci Forum, 2007; 546–549: 1551[2] Chawla N. Adv Mater Process, 2006; 164(7): 29[3] Rawal S. J Met, 2001; 53(4): 14[4] Chawla N, Chawla K K. J Met, 2006; 58(11): 67[5] Evans R D, Boyd J D. Scr Mater, 2003; 49: 59[6] Zhou J, Dru˙zd˙zel A T, Duszczyk J. J Mater Sci, 1999; 34: 5089[7] Gupta A K. Bull Mater Sci, 1995; 18: 773[8] Geng L, Qu S J, Lei T Q. Key Eng Mater, 2003; 249: 233[9] Savitskii A P, Romanov G N, Marisunova L S. Russ Phys J, 1968; 11(8): 5[10] Savitskii A P, Romanov G N. Powder Metall Met Ceram, 1986; 25: 184[11] Min K H, Kang S P, Lee B H, Lee J K, Kim Y D. J Alloys Compd, 2006; 419: 290[12] Rahimian M, Ehsani N, Parvin N, Baharvandi H R. J Mater Process Technol, 2009; 209: 5387[13] Hong S H, Chung K H. Mater Sci Eng, 1995; A194: 165[14] Song M, He Y H. Mater Des, 2010; 31: 985[15] Min K H, Kang S P, Kim D G, Kim Y D. J Alloys Compd, 2005; 400: 150[16] Fogagnolo J B, Robert M H, Torralba J M. Mater Sci Eng, 2006; A426: 85[17] Shin K S, Chung D S, Lee S H. Metall Mater Trans, 1997; 28A: 2625[18] Laurent V, Chatain D, Eustathopoulos N. Mater Sci Eng, 1991; A135: 894[19] Gu M Y, Mei Z, Jin Y P, Wu Z A. Scr Mater, 1999; 40: 985[20] Shi Z L, Ochiai S, Hojo M, Lee J C, Gu M Y, Lee H, Wu R J. J Mater Sci, 2001; 36: 2441[21] Luo Z P, Song Y G, Zhang S Q. Scr Mater, 2001; 45: 1183[22] Wang N, Wang Z R, Weatherly G C. Metall Trans, 1992; 23A: 1423[23] RatnaParkhi P L, Howe J M. Metall Mater Trans, 1994; 25A: 617[24] Zhong W M, Esperance G L, Suery M. Metall Mater Trans, 1995; 26A: 2637[25] Gonzalez G, Salvo L, Suery M, L’Esp´erance G. Scr Metall Mater, 1995; 33: 1969[26] Wang N, Wang Z, Weatherly G C. Metall Trans, 1979; 23A: 1423[27] Kim Y M, Lee J C. Mater Sci Eng, 2006; A420: 8[28] Carotenuto G, Gallo A, Nicolais L. J Mater Sci, 1994; 29: 4967[29] Lloyd D J, Lagaoe H, McLeod A, Morris P L. Mater Sci Eng, 1989; A107: 73[30] Sahin Y. Mater Des, 2006; 24: 671[31] Carim A H. Mater Lett, 1991; 12: 153[32] Man C F, Mummery P M, Derby B, Jenkins M L. In: Frank J ed., Proc 2nd Int Conf Interfacial Phenomena in Composite Materials, Leuven: Butterworth–Heinemann,1991: 175[33] Thebaud F, Herve E, Silva R D, Suery M, Bretheau T. In: Frank J ed., Proc 2nd Int Conf Interfacial Phenomena in Composite Materials, Leuven: Butterworth–Heinemann,1991: 179 |
|