Fe3C和珠光体对低碳铁素体钢腐蚀电化学行为的影响 |
王力伟,杜翠薇,刘智勇,曾笑笑,李晓刚 |
北京科技大学腐蚀与防护中心教育部腐蚀与防护重点实验室, 北京 100083 |
|
INFLUENCES OF Fe3C AND PEARLITE ON THE ELECTROCHEMICAL CORROSION BEHAVIORS OF LOW CARBON FERRITE STEEL |
WANG Liwei, DU Cuiwei, LIU Zhiyong, ZENG Xiaoxiao, LI Xiaogang |
Key Laboratory of Corrosion and Protection, Ministry of Education of China, Corrosion and Protection Center, University
of Science and Technology Beijing, Beijing 100083 |
引用本文:
王力伟 杜翠薇 刘智勇 曾笑笑 李晓刚. Fe3C和珠光体对低碳铁素体钢腐蚀电化学行为的影响[J]. 金属学报, 2011, 47(10): 1227-1232.
,
,
,
,
.
INFLUENCES OF Fe3C AND PEARLITE ON THE ELECTROCHEMICAL CORROSION BEHAVIORS OF LOW CARBON FERRITE STEEL[J]. Acta Metall Sin, 2011, 47(10): 1227-1232.
[1] Carneiro R A, Ratnapuli R C, de Freitas Cunha Lins V. Mater Sci Eng, 2003; A357: 104[2] Gonzalez–Rodriguez J G, Casales M, Salinas–Bravo V M. Corrosion, 2002; 58: 584[3] Chu R, Chen W, Wang S H. Corrosion, 2004; 60: 275[4] Bulger J T, Lu BT, Luo J L. J Mater Sci, 2006; 41: 5001[5] Albarran J L, Martinez L, Lopez H F. Corros Sci, 1999; 41: 1037[6] Lee S, Kim B, Kwon D. Metall Mater Trans, 1992; 23A: 2803[7] Liu Z Y, Li X G, Du C W. Corros Sci, 2009; 51: 895[8] Kobayashi Y, Ume K, Hyodo T. Corros Sci, 1987; 27: 1117[9] Fan Z, Liu J Y, Li S L, Zhang T J. J Southwest Petro Univ (Sci Technol Ed), 2009; 31: 171(范舟, 刘建仪, 李士伦, 张天江. 西南石油大学学报(自然科学版), 2009; 31: 171)[10] Santos T F A, Hermenegildo T F C, Afonso C R M. Eng Fract Mech, 2010; 77: 2937[11] Ale R M, Rebello J M A, Charlier J. Mater Charact, 1996; 37: 89[12] Xue X H, Zhou Y, Qian B N, Li J L, Lou S N. J Shanghai Jiaotong Univ, 2003; 37: 1854(薛小怀, 周 昀, 钱百年, 李晶丽, 楼松年. 上海交通大学学报, 2003; 37: 1854)[13] Souto R M, Gonzalez–Garcia Y, Bastos A C. Corros Sci, 2007; 49: 4568[14] Simôes A M, Bastos A C, Souto R M. Corros Sci, 2007; 49: 726[15] Krawiec H, Vignal V, Oltra R. Electrochem Commun, 2004; 6: 655[16] Annergren I, Zou F, Thierry D. Electrochim Acta, 1999; 44: 4383[17] Tang X, Cheng Y F. Appl Surf Sci, 2008; 254: 5199[18] Zou F, Dominigue T, Han W A. Corros Sci Protect Technol, 1997; 9: 276(邹锋, Dominigue T, 韩文安. 腐蚀科学与防护技术, 1997; 9: 276)[19] Zhang G A, Cheng Y F. Corros Sci, 2009; 51: 1714[20] ASM Committee on Gas Carburizing. Carburizing and Carbonitriding. Ohio: American Society for Metals, 1977: 179[21] Liu Z Y, Li X G, Du C W. Corros Sci, 2009; 51: 2863[22] Ohnori Y. Trans ISIJ, 1972; 12: 128[23] Stratmann M. Corros Sci, 1987; 27: 869[24] Stratmann M, Streckel H, Bunsen B. Phys Chem, 1988, 92: 1244[25] Park C J, Kwon H S. Corros Sci, 2002; 44: 2817[26] Lo I H, Fu Y, Lin C J. Corros Sci, 2006; 48: 696[27] Liu Z Y, Li X G, Du C W. Corros Sci, 2009; 51: 895[28] Liu X, Mao X. Scr Mater, 1995; 33: 145[29] Clover D, Kinsella B, Pejcic B. J Appl Electrochem, 2005; 35: 139[30] Liu Z Y, Zhai G L, Du C W, Li X G. Acta Metall Sin, 2008; 44: 209(刘智勇, 翟国丽, 杜翠薇, 李晓刚. 金属学报, 2008; 44: 209) |
|