| 显微组织对TC4ELI合金疲劳裂纹扩展路径及扩展速率的影响 |
| 马英杰1), 李晋伟2), 雷家峰1), 唐振云2), 刘羽寅1), 杨锐1) |
1) 中国科学院金属研究所, 沈阳 110016
2) 中航工业北京航空制造工程研究所, 北京 100024 |
|
| INFLUENCES OF MICROSTRUCTURE ON FATIGUE CRACK PROPAGATING PATH AND CRACK GROWTH RATES IN TC4ELI ALLOY |
| MA Yingjie1), LI Jinwei2), LEI Jiafeng1), TANG Zhenyun2), LIU Yuyin1), YANG Rui1) |
1) Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
2) AVIC Beijing Aeronautical Manufacturing Technology Research Institute, Beijing 100024 |
引用本文:
马英杰 李晋伟 雷家峰 唐振云 刘羽寅 杨锐. 显微组织对TC4ELI合金疲劳裂纹扩展路径及扩展速率的影响[J]. 金属学报, 2010, 46(9): 1086-1092.
,
,
,
,
.
INFLUENCES OF MICROSTRUCTURE ON FATIGUE CRACK PROPAGATING PATH AND CRACK GROWTH RATES IN TC4ELI ALLOY[J]. Acta Metall Sin, 2010, 46(9): 1086-1092.
| [1]Sinha V, Soboyejo W O. Mater Sci Eng A, 2001; 319-321: 607
[2]Sansoz F, Ghonem H. Mater Sci Eng A, 2003; 356: 81
[3]Lindigkeit J, Terlinde G, Gysler A, Lütjering G. Acta Metall, 1979; 27: 1717
[4]Carter R D, Lee E W, Starke E A, Beevers C. J Met Trans, 1984; 15A: 555
[5]Suresh S, Fatigue Met Trans A, 1985; 16: 249
[6]Suresh S. Translated by Wang Z G, Zang Q Sh, Li Sh X. Fatigue of Material. Beijing: Defense Industrial Press, 1999: 355
(Suresh S著, 王中光, 臧启山, 李守新译. 材料的疲劳, 北京: 国防工业出版社, 1999: 355)
[7]Goswami T. Mater Design. 2003; 24: 423
[8]Ding J, Hall R, Byrne J. Int J Fatigue. 2005; 27: 1551
[9]Shademan S, Sinha V, Soboyejo A B O, Soboyejo W O. Mech of Mater, 2004; 36: 161
[10]Jata K V, Starke E A. J Met Trans A, 1986; 17A: 1011
[11]Suresh S, Zamiski G F, Ritchie R O. Met Trans A, 1981; 12A: 1435
[12]Vasudevan A K, Suresh S. Met Trans A, 1982; 13A: 2271
[13]Lütjering G. Mater Sci Eng A, 1998; 243: 32.
[14]Lütjering G. Mater Sci Eng A, 1999; 263: 117
[15]Filip R, Kubiak K, Ziaja W, Sieniawski J. J Mater Processing Tech, 2003; 133: 84
[16]Li Sh K, Xiong B Q, Hui S X, Ye W J, Yu Y. Mater Sci Eng A, 2007; 460–461: 140
[17]Ma Y J, Liu J R, Lei J F, Liu Y Y, Yang R. Chinese J Mater Research, 2008; 22: 555
(马英杰, 刘建荣, 雷家峰, 刘羽寅, 杨锐. 材料研究学报, 2008; 22: 555)
[18]Gil F J, Planell J A. Mater Sci Eng A, 2000; 283: 17
[19]Semiatin S L, Fagin P N, Glavicic M G, Ivasishin O M. Mater Sci Eng A, 2001; 299: 225
[20]Semiatin S L, Soper J C, Sukonnik I M. Scri Met Meterialia, 1994; 30: 951
[21]Борисова E A. Translated by Chen Sh Q. Metallography of Titanium Alloy. Beijing: Defense Industrial Press, 1986: 235
(鲍利索娃E A 著. 陈石卿译. 钛合金金相学. 北京:国防工业出版社,1986: 235).
[22]Ma Y J, Liu J R, Lei J F, Liu Y Y, Yang R. Rare Met Mater Eng, 2009; 38: 976
(马英杰, 刘建荣, 雷家峰, 刘羽寅, 杨锐. 稀有金属材料与工程, 2009; 38: 976)
[23]Ma Y J, Liu J R, Lei J F, Li Y R, Liu Y Y, Yang R. Acta Metall Sin, 2008; 44: 973
(马英杰, 刘建荣, 雷家峰, 李玉兰, 刘羽寅, 杨锐. 金属学报, 2008; 44: 973)
[24]Ma Y J, Liu J R, Lei J F, Liu Y Y, Yang R. Rare Met Mater Eng, 2008; 37(suppl): 633
(马英杰, 刘建荣, 雷家峰, 刘羽寅,杨锐. 稀有金属材料与工程, 2008; 37(suppl): 633)
[25]Xu F. PhD Thesis, Institute of Metal Research CAS, 2008
(徐峰, 博士学位论文, 中国科学院金属研究所, 2008)
[26]Savage M F. Mater Sci Eng A, 2001; 319–321: 398
[27]Sansoz F, Ghonem H. Mater Sci Eng A, 2003; 356: 81
[28]Li Sh K, Xiong B Q, Hui S X, Ye W J, Yu Y. Mater Characterization, 2008; 59: 397
[29]Schroeder G, Albrecht J, Luetjering G. Mater Sci Eng A, 2001; 319–321: 602
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|