| 激光立体成形Ti-80%Ni合金显微组织及力学性能 |
| 许小静1, 2), 林鑫1), 黄卫东1), 王亮2) |
1) 西北工业大学凝固技术国家重点实验室, 西安 710072
2) 航天材料及工艺研究所, 北京 100076 |
|
| MICROSTRUCTURE AND MECHANICAL PROPERTY OF Ti-80%Ni ALLOY PREPARED BY LASER SOLID FORMING |
| XU Xiaojing1, 2), LIN Xin1), HUANG Weidong1), WANG Liang2) |
1) State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072
2) Aerospace Research Institute of Materials & Processing Technology, Beijing 100076 |
引用本文:
许小静 林鑫 黄卫东 王亮. 激光立体成形Ti-80%Ni合金显微组织及力学性能[J]. 金属学报, 2010, 46(9): 1081-1085.
,
,
.
MICROSTRUCTURE AND MECHANICAL PROPERTY OF Ti-80%Ni ALLOY PREPARED BY LASER SOLID FORMING[J]. Acta Metall Sin, 2010, 46(9): 1081-1085.
| [1] Chen B Y. Aero Sci Technol, 1998; 2:13
(陈炳贻. 航空科学技术, 1998; 2: 13)
[2] Suryanarayana C, Fores F H, Rowe R G. Int Mater Rev, 1991; 36: 85
[3] Abbott D H, Arcella F G. Adv Mater Process, 1998; 5: 29
[4] Baughman M S. Rapid Prototyping J, 2005; 11: 41
[5] Lin X, Yue T M, Yang H O, Huang W D. Acta Mater, 2006; 54: 1901
[6] Huang W D, Lin X, Chen J, Liu Z X, Li Y M. Laser Solid Forming. Beijing: National Defense Industry Press, 2007: 107
(黄卫东, 林 鑫, 陈 静, 刘振侠, 李延民. 激光立体成形. 北京: 国防工业出版社, 2007: 107)
[7] Krishnamurthy S, Froes F H. Int Mater Rev, 1989; 34: 297
[8] Radojevic B. Mater Sci Eng, 2001; A304–306: 385
[9] Otsuka K, Ren X. Prog Mater Sci, 2005; 50: 516
[10] Nagarajan R, Ranganathan S, Aoki K, Chattopadhyay K. Mater Trans, JIM, 1997; 138: 406
[11] Li Y M. PhD Thesis, Northwestern Polytechnical University, Xi’an, 2001
(李延民. 西北工业大学博士学位论文, 西安, 2001)
[12] Li Y M, Li J G, Yang H O, Lin X, Chen J, Huang W D. Appl Laser, 2002; 22: 140
(李延民, 李建国, 杨海欧, 林鑫, 陈静, 黄卫东. 应用激光, 2002; 22: 140)
[13] Huang W D, Li Y M, Feng L P, Chen J, Yang H O, Lin X. J Mater Eng, 2002; 3: 40
(黄卫东, 李延民, 冯丽萍, 陈 静, 杨海欧, 林鑫. 材料工程, 2002; 3: 40)
[14] Trived R, Somboonsuk K. Mater Sci Eng, 1984; 65: 65
[15] Kurz W, Fisher D J. Fundamentals of Solidification. Aedermannsdorf, Switzerland: Trans. Tech. 1981: 36 |
|