| DZ417G镍基定向凝固高温合金的再结晶 |
| 彭胜,周兰章,侯介山,郭建亭 |
| 中国科学院金属研究所, 沈阳 110016 |
|
| THE RECRYSTALLIZATION OF Ni BASE DIRECTIONALLY SOLIDIFIED SUPERALLOY DZ417G |
| PENG Sheng, ZHOU Lanzhang, HOU Jieshan, GUO Jianting |
| Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
彭胜 周兰章 侯介山 郭建亭. DZ417G镍基定向凝固高温合金的再结晶[J]. 金属学报, 2010, 46(8): 907-912.
,
,
.
THE RECRYSTALLIZATION OF Ni BASE DIRECTIONALLY SOLIDIFIED SUPERALLOY DZ417G[J]. Acta Metall Sin, 2010, 46(8): 907-912.
| [1] Wang D L, Li J B, Jin T, Yang S Q, Wei Z, Hu Z Q, Fu L Q. Acta Metall Sin, 2006; 42: 167
(王东林, 李家宝, 金涛, 杨胜群, 魏政, 胡壮麒, 付立群. 金属学报, 2006; 42: 167)
[2] Xie G, Wang L, Zhang J, Lou L H. Metall Mater Trans, 2008; 39A: 206
[3] Marsden P K. J Mater Sci, 1971; 6: 1038
[4] Wang L, Xie G, Zhang J, Lou L H. Scr Mater, 2006; 55: 457
[5] Porter A, Ralph B. J Mater Sci, 1981; 16: 707
[6] Bond S D, Martin J W. J Mater Sci, 1984; 19: 3867
[7] Jo C Y, Cho H Y, Kim H M. Mater Sci Technol, 2003; 19: 1665
[8] Cox D C, Roebuck B, Rae C M F, Reed R C. Mater Sci Technol, 2003; 19: 440
[9] Zambaldi C, Roters F, Raabe D, Glatzel U. Mater Sci Eng, 2007; A454–455: 433
[10] Zhao Y,Wang L, Yu T, Ding H F. Rare Metall Mater Eng, 2008; 37: 1032
[11] Xiong J C, Li J R, Zhao J Q, Liu S Z, Dong J X. Acta Metall Sin, 2009; 45: 1232
(熊继春, 李嘉荣, 赵金乾, 刘世忠, 董建新. 金属学报, 2009; 45: 1232)
[12] Zhang B, Tao C H, Lu X, Liu C K, Hu C Y, Bai M Y. J Iron Steel Res Int, 2009; 16: 75
[13] Xie G, Zhang J, Lou L H. Scr Mater, 2008; 59: 858
[14] B¨urgel R, Portella P D, Preuhs J. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, McLean M, Olson S, Schirra J J, eds., Superalloys 2000, Seven Spring, PA: TMS, 2000: 229
[15] Gostic W J. US Pat, 5551999, 1996
[16] Mihalisin J R, Corrigan J, Gratti G M, Vogt R G. US Pat, 2002/0007877 A1, 2002
[17] Keiichi M. Euro Pat, 1036850 A1, 2000
[18] Zoltzer K, Lempenauer K, Fischmeister H. US Pat, 5294239, 1994
[19] Corrigan J, Vogt R G, Mihalisin J R, Schmiedeknecht D L. Euro Pat, 1038982 A1, 1999
[20] Salkeld R W, Field T T, Ault E A. US Pat, 5413648, 1995
[21] Okazaki M, Ohtera I, Harada Y. Metall Mater Trans, 2004; 35A: 535
[22] Zhang W F , Li Y J, Liu G Y, Zhao A G, Tao C H, Tian J F, Yao G. Eng Fail Anal, 2000; 11: 429
[23] Zhao Y, Wang L, Li H Y, Yu T, Liu Y. Rare Met, 2008; 27: 425
[24] Jo C Y, Cho H Y, Kim H M. Mater Sci Technol, 2003; 19: 1671
[25] Li Y J, Zhang W F, Tao C H. J Mech Strength, 2006; 28: 135
(李运菊, 张卫方, 陶春虎. 机械强度, 2006; 28: 135)
[26] Li Y J, Tao C H, Zhang W F. Adv Eng Mater, 2007; 9: 867
[27] Xie G, Wang L, Zhang J, Lou L H. In: Reed R C, Green K A, Caron P, Gabb T P, Fahrmann M G, Huron E S, Woodard S A, eds., Superalloys 2008, Seven Spring, PA: TMS, 2008: 453
[28] Paul U, Sahm P R. Mater Sci Eng, 1993; A173: 49
[29] Guo J T, Yuan C, Yang H C, Lupinc V, Maldini M. Metall Mater Trans, 2001; 32A: 1103 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|