| 热镀锌TRIP钢中马氏体对力学性能的影响 |
| 定巍 唐荻 江海涛 黄伟 |
| 北京科技大学高效轧制国家工程研究中心; 北京 100083 |
|
| INFLUENCE OF MARTENSITE ON MECHANICAL PROPERTIES OF HOT-DIP GALVANIZED TRIP STEEL |
| DING Wei; TANG Di; JIANG Haitao; HUANG Wei |
| National Engineering Research Center for Advanced Rolling Technology; University of Science & Technology Beijing; Beijing 100083 |
引用本文:
定巍 唐荻 江海涛 黄伟. 热镀锌TRIP钢中马氏体对力学性能的影响[J]. 金属学报, 2010, 46(5): 595-599.
,
,
,
.
INFLUENCE OF MARTENSITE ON MECHANICAL PROPERTIES OF HOT-DIP GALVANIZED TRIP STEEL[J]. Acta Metall Sin, 2010, 46(5): 595-599.
| [1] Tang D, Mi Z L, Cheng Y L. Iron Steel, 2005; 40(6): 1
(唐 荻, 米振莉, 陈雨来. 钢铁, 2005; 40(6): 1)
[2] Zhang Q F, Liu B J, Huang J Z. Modern Continuous Hot Dip Galvanizing of Steel Sheets. Beijing: Metallurgy Industry Press, 2007: 587
(张启富, 刘邦津, 黄建中.现代带钢连续热镀锌. 北京: 冶金工业出版社, 2007: 587)
[3] Zackay V F, Parker E R, Fahr D, Busch R A. Trans ASM, 1967; 60: 252
[4] Matsumura O, Sakuma Y, Takechi H. Scr Metall, 1987; 21: 1301
[5] Jiang H T, Wu H B, Tang D, Liu Q. J Univ Sci Technol Beijing, 2008; 15: 574
[6] Qi J J, Huang Y H, Zhang Y. Microalloyed Steel. Beijing: Metallurgy Industry Press, 2006: 70
(齐俊杰, 黄云华, 张跃. 微合金化钢. 北京: 冶金工业出版社, 2006: 70)
[7] Zhou Y, Wu G H. Analysis Methods in Materials Science. Harbin: Harbin Institute Technology Press, 2007: 95
(周玉, 武高辉. 材料分析测试技术. 哈尔滨: 哈尔滨工业大学出版社, 2007: 95)
[8] Liesbeth B. PhD Thesis, Ghent University, Belgium, 2006
[9] De Cooman B C. Curr Opinion Solid State Mater Sci, 2004; 8: 285
[10] Koistinen D P, Marburger R E. Acta Metall, 1959; 7: 59
[11] Sugimoto K I, Sakaguchi J, Tsutomu I, Kashima T. ISIJ Int, 2000; 4: 920
[12] Speich G R, Demarest V A, Miller R L. Metall Mater Trans, 1981; 12A: 1419
[13] Gilmour J B, Purdy G R, Kirkaldy J S. Metall Mater Trans, 1972; 6A: 1455
[14] Jacques P J, Girault E, Mertens A, Verlinden B, Humbeeck J V, Delannay F. ISIJ Int, 2001; 41: 1068
[15] Kim S J, Lee C G, Lee T H, Oh C S. Scr Mater, 2003; 48: 539 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|