|
|
|
| 等通道转角挤压过程中fcc金属的微观结构演化与力学性能 |
| 吴世丁; 安祥海; 韩卫忠; 屈伸; 张哲峰 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室; 沈阳 110016 |
|
| MICROSTRUCTURE EVOLUTION AND MECHANICAL PROPERTIES OF FCC METALLIC MATERIALS SUBJECTED TO EQUAL CHANNEL ANGULAR PRESSING |
| WU Shiding; AN Xianghai; HAN Weizhong; QU Shen; ZHANG Zhefeng |
| Shenyang National Laboratory for Materials Science; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
吴世丁 安祥海 韩卫忠 屈伸 张哲峰. 等通道转角挤压过程中fcc金属的微观结构演化与力学性能[J]. 金属学报, 2010, 46(3): 257-276.
,
,
,
,
.
MICROSTRUCTURE EVOLUTION AND MECHANICAL PROPERTIES OF FCC METALLIC MATERIALS SUBJECTED TO EQUAL CHANNEL ANGULAR PRESSING[J]. Acta Metall Sin, 2010, 46(3): 257-276.
| [1] Gleiter H. Prog Mater Sci, 1989; 33: 223
[2] Valiev R Z, Islamgaliev R K, Alexandrov I V. Prog Mater Sci, 2000; 45: 103
[3] Valiev R Z, Langdon T G. Prog Mater Sci, 2006; 51: 881
[4] Valiev R Z, Korznikov A V, Mulyukov R R. Mater Sci Eng, 1993; A168: 141
[5] Torre F D, Lapovok R, Sandlin J, Thomson P F, Davies C H J, Pereloma E V. Acta Mater, 2004; 52: 4819
[6] Zhilyaev A P, Langdon T G. Prog Mater Sci, 2008; 53: 893
[7] Saito Y, Utsunomiya H, Tsuji N, Sakai T. Acta Mater, 1999; 47: 579
[8] Li Y S, Tao N R, Lu K. Acta Mater, 2008; 56: 230
[9] Cui G R, Ma Z Y, Li S X. Acta Mater, 2009; 57: 5718
[10] Segal V M. Mater Sci Eng, 1995; A197: 157
[11] Segal V M. Mater Sci Eng, 2003; A345: 36
[12] Wang Z G, Wu S D, Jiang C B, Liu S M, Alexandrov I V. Proc Fatigue, vol.3, West Midlands: Engineering Advisory Services, 2002: 1541
[13] Fukuda Y, Oh-ishi K, Furukawa M, Horita Z, Langdon T G. Mater Sci Eng, 2006; A420: 79
[14] Fukuda Y, Oh-ishi K, Furukawa M, Horita Z, Langdon T G. Acta Mater, 2004; 52: 1387
[15] Miyamoto H, Erb U, Koyama T, Mimaki T, Vinogradov A, Hashimoto S. Philos Mag Lett, 2004; 84: 235
[16] Zhu Y T, Lowe T C. Mater Sci Eng, 2000; A291: 46
[17] Iwahashi Y, Horita Z, Nemoto M, Langdon T G. Acta Mater, 1997; 45: 4733
[18] Iwahashi Y, Horita Z, Nemoto M, Langdon T G. Acta Mater, 1998; 46: 3317
[19] Tao N R, Lu K. Scr Mater, 2009; 60: 1039
[20] An X H, Han W Z, Huang C X, Zhang P, Yang G, Wu S D, Zhang Z F. Appl Phys Lett, 2008; 92: 201915
[21] Wang Y M, Ma E. Acta Mater, 2004; 52: 1699
[22] Zhao Y H, Zhu Y T, Liao X Z, Horita Z, Langdon T G. Appl Phys Lett, 2006; 89: 121906
[23] Han W Z. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2008
(韩卫忠. 中国科学院金属研究所博士论文, 沈阳, 2008)
[24] Qu S. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2009
(屈伸. 中国科学院金属研究所博士论文, 沈阳, 2009)
[25] An X H, Lin Q Y, Qu S, Yang G, Wu S D, Zhang Z F. J
Mater Res, 2009: 24: 3636
[26] An X H, Qu S, Wu S D, Zhang Z F. J Mater Res, submitted
[27] Han W Z, Zhang Z F, Wu S D, Li S X. Acta Mater, 2007;
55: 5889
[28] Han W Z, Yang H J, An X H, Yang R Q, Li S X, Wu S
D, Zhang Z F. Acta Mater, 2009; 57: 1132
[29] Zhang Z F, Wang Z G. Acta Mater, 2003; 51: 347
[30] Zhang Z F, Wang Z G. Prog Mater Sci, 2008; 53: 1025
[31] Yamakov V, Wolf D, Phillpot S R, Mukherjee A K, Gleiter
H. Acta Mater, 2001; 49: 2713
[32] Han W Z, Zhang Z F, Wu S D, Li S X. Philos Mag, 2008;
88: 3011
[33] Han W Z, Wu S D, Li S X, Zhang Z F. Appl Phys Lett,
2008; 92: 221909
[34] Han W Z, Cheng G M, Li S X, Wu S D, Zhang Z F. Phys
Rev Lett, 2008; 101: 115505
[35] Han W Z, Wu S D, Huang C X, Li S X, Zhang Z F. Adv
Eng Mater, 2008; 10: 1110
[36] Christian J W, Mahajan S. Prog Mater Sci, 1995; 39: 1
[37] Venables J A. Philos Mag, 1961; 6: 379
[38] Hang C X, Wang K, Wu S D, Zhang Z F, Li G Y, Li S X.
Acta Mater, 2006; 54: 655
[39] Hirth J P, Lothe J. Theory of Dislocations. 2 Ed., John
Wiley & Son Inc., Canada, 1982: 1
[40] Shan Z W, Stach E A, Wiezorek J M K, Knapp J A, Follstaedt
D M, Mao S X. Science, 2004; 305: 654
[41] Van Swygenhoven H. Science, 2002; 296: 66
[42] Qu S, An X H, Yang H J, Huang C X, Yang G, Zang Q
S, Wang Z G, Wu S D, Zhang Z F. Acta Mater, 2009; 57:
1586
[43] Komura S, Horita Z, Nemoto M. J Mater Res, 1999; 14:
4044
[44] Zhilyaev A P, Kim B K, Szpunar J A. Mater Sci Eng,
2005; A391: 377
[45] Mohamed F A. Acta Mater, 2003; 51: 4107
[46] Balogh L, Ung´ar T, Zhao Y H, Zhu Y T, Horita Z, Xu C,
Langdon T G. Acta Mater, 2008; 56: 809
[47] Lu L, Shen Y, Chen X, Qian L, Lu K. Science, 2004; 304:
422
[48] Lu L, Chen X, Huang X, Lu K. Science, 2009; 323: 607
[49] Shen Y, Lu L, Lu Q H, Jin Z H, Lu K. Scr Mater, 2005;
52: 989
[50] Li Y S, Zhang Y, Tao N R, Lu K. Acta Mater, 2009; 57:
761 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|