| 珠光体钢丝冷拉拔过程中微观组织及铁素体微区取向与织构演变 |
| 张晓丹1;A Godfrey 1;刘伟1;刘庆2 |
1.清华大学材料科学与工程系; 北京 100084
2.重庆大学材料学院; 重庆 400044 |
|
| EVOLUTIONS OF MICROSTRUCTURE AND FERRITIC MICRO–ORIENTATION AND TEXTURE IN A PEARLITIC STEEL WIRE DURING COLD DRAWING |
| ZHANG Xiaodan1; A. Godfrey1; LIU Wei1;LIU Qing2 |
1.Department of Materials Science and Engineering; Tsinghua University; Beijing 100084
2.School of Materials Science and Engineering; Chongqing University; Chongqing 400044 |
引用本文:
张晓丹 A Godfrey 刘伟 刘庆. 珠光体钢丝冷拉拔过程中微观组织及铁素体微区取向与织构演变[J]. 金属学报, 2010, 46(2): 141-146.
,
,
,
.
EVOLUTIONS OF MICROSTRUCTURE AND FERRITIC MICRO–ORIENTATION AND TEXTURE IN A PEARLITIC STEEL WIRE DURING COLD DRAWING[J]. Acta Metall Sin, 2010, 46(2): 141-146.
| [1] Ochiai M, Nishida S, Ohba H, Kawata H. J Iron Steel Inst, 1993; 79: 89
[2] Zelin M. Acta Mater, 2002; 50: 4431
[3] Heizmann J J, Tidu A, Bolle B, Peeters L. Wire J Int, 1999; 32(7): 150
[4] Liu Y D, Jiang Q W, Wang G, Wang Y D, Tidu A, Zuo L. J Mater Sci Technol, 2005; 21: 357
[5] VanEssen C G, Schulson E M, Donaghay R H. Nature, 1970; 225: 847
[6] Joy D C, Newbury D E, Davidson D L. J Appl Phys, 1982; 53: 81
[7] Adams B L, Dingley D J, Kunze K, Wright S I. Mater Sci Forum, 1994; 157–162: 31
[8] Hurley P J, Humphreys F J. Acta Mater, 2003; 51: 1087
[9] Jensen J D. Acta Metall Mater, 1995; 43: 4117
[10] Li B L, Godfrey A, Liu Q. Mater Sci Forum, 2002; 408–412: 1185
[11] Yao Z Y, Liu Q, Godfrey A, LiuW. Acta Metall Sin, 2009; 45: 641
(姚宗勇, 刘 庆, Godfrey A, 刘伟. 金属学报, 2009; 45: 641)
[12] Huges D A, Hansen N. Metall Trans, 1993; 24A: 2021
[13] Houtte P V,Watte P, Aernoudt E, Sevillano J G, Lefever I, Raemdonck W V. Mater Sci Forum, 1994; 157–162: 1881
[14] Liu Y D, Jiang Q W, Zhao X, Zuo L, Liang Z D. Acta Metall Sin, 2002; 38: 1215
(刘沿东, 蒋奇武, 赵骧, 左良, 梁志德. 金属学报, 2002; 38: 1215)
[15] Walentek A, Seefeldt M, Verlinden B, Aernoudt E, Van Houtte P. J Microscopy, 2006; 224: 256
[16] Walentek A, Seefeldt M, Verlinden B, Aernoudt E, Van Houtte P. Mater Sci Eng, 2008; A483–484: 716
[17] Li S, Yip T H, Ramanujan R V, Liang M H. Mater Sci Technol, 2003; 19: 902 |
|