| 包Al层聚集对搅拌摩擦焊接头力学性能的影响 |
| 康旭1,史清宇1,孙凯1,王鑫2 |
1.清华大学机械工程系先进成形制造教育部重点实验室, 北京 100084
2. 清华大学核能与新能源技术研究院, 北京 100084 |
|
| INFLUENCES ON MECHANICAL PROPERTIES OF FRICTION STIR WELDED JOINTS BY Al CLAD ACCUMULATION |
| KANG Xu1, SHI Qingyu1, SUN Kai1, WANG Xin2 |
1.Key Laboratory for Advanced Materials Processing Technology, Department of Mechanical Engineering, Tsinghua
University, Beijing 100084
2.Institute of Nuclear and New Energy Technology, Tsinghua University, Beijing 100084 |
引用本文:
康旭 史清宇 孙凯 王鑫. 包Al层聚集对搅拌摩擦焊接头力学性能的影响[J]. 金属学报, 2010, 46(12): 1517-1521.
,
,
,
.
INFLUENCES ON MECHANICAL PROPERTIES OF FRICTION STIR WELDED JOINTS BY Al CLAD ACCUMULATION[J]. Acta Metall Sin, 2010, 46(12): 1517-1521.
| [1] Thomas W M, Nicholas E D, Needham J C, Murch M G, Templesmith P, Dawes C J. Gr Br Pat Appl No. 9125978.8, 1991
[2] Mishra R S, Ma Z Y. Mater Sci Eng, 2005; R50: 1
[3] Colegrove P A, Shercliff H R. Sci Technol Weld Joining, 2003; 8(5): 360
[4] Threadgill P L, Leonard A J, Shercliff H R, Withers P J. Int Mater Rev, 2009; 54(2): 49
[5] Lombard H, Hattingh D G, Steuwer A, James M N. Eng Fract Mech, 2008; 75: 341
[6] Zhou P Z, Li D H, He D Q, Deng H. Trans Chin Weld Inst, 2007; 28(10): 5
(周鹏展, 李东辉, 贺地求, 邓航. 焊接学报, 2007; 28(10): 5)
[7] Wang W, Shi Q Y, Li T, Li Hong Ke. Trans Chin Weld Inst, 2008; 29(5): 77
(王伟, 史清宇, 李亭, 李红克. 焊接学报, 2008; 29(5): 77)
[8] Zhao J J, Zhang P, Wang W X, Ma L, Hu W W. Trans Chin Weld Inst, 2005; 26(5): 61
(赵军军, 张平, 王卫欣, 马琳, 胡卫伍. 焊接学报, 2005; 26(5): 61)
[9] Fu Z H, He D Q, Zhou P Z, Hu A W. Trans Chin Weld Inst, 2006; 27(5): 65
(傅志红, 贺地求, 周鹏展, 胡爱武. 焊接学报, 2006; 27(5): 65)
[10] Zhou P Z, Zhong J, He D Q. Chin J Nonferr Metals, 2006; 16(6): 964
(周鹏展, 钟掘, 贺地求. 中国有色金属学报, 2006; 16(6): 964)
[11] Elangovan K, Balasubramanian V. Mater Des, 2008; 29: 362
[12] Ke L M, Pan J L, Xing L, Wang S L. Trans Chin Weld Inst, 2007; 28(5): 33
(柯黎明, 潘际銮, 邢丽, 王善林. 焊接学报, 2007; 28(5): 33)
[13] Dong C L, Shen C B, Wang Z Z. J Dalian Jiaotong Univ, 2009; 30(6): 42
(董春林, 沈长斌, 王忠志. 大连交通大学学报, 2009; 30(6): 42)
[14] Yan K, Ma Z X, Zhang J. J Mater Eng, 2008; 9: 44
(严铿, 马志新, 张健. 材料工程, 2008; 9: 44)
[15] Kang X. Bachelor Thesis, Tsinghua University, Beijing, 2008
(康旭. 清华大学学士学位论文, 北京, 2008)
[16] Wang X. Master Thesis, Tsinghua University, Beijing, 2008
(王鑫. 清华大学硕士学位论文, 北京, 2009)
|
|