| 轨道交通车辆用6005A合金板材时效析出及硬化行为研究 |
| 杨文超1,汪明朴1,盛晓菲1,张茜1,王正安2 |
1.中南大学材料科学与工程学院, 长沙 410083
2.中南大学教育部有色金属材料科学与工程实验室, 长沙 410083 |
|
| STUDY OF THE AGING PRECIPITATION AND HARDENING BEHAVIOR OF 6005A ALLOY SHEET FOR RAIL TRAFFIC VEHICLE |
| YANG Wenchao1, WANG Mingpu1, SHENG Xiaofei1, ZHANG Qian1, WANG Zheng’an2 |
1.School of Materials Science and Engineering, Central South University, Changsha 410083
2.Key laboratory of Nonferrous Metal Materials Science and Engineering, Ministry of Education, Central South University,
Changsha 410083 |
引用本文:
杨文超 汪明朴 盛晓菲 张茜 王正安. 轨道交通车辆用6005A合金板材时效析出及硬化行为研究[J]. 金属学报, 2010, 46(12): 1481-1487.
,
,
,
,
.
STUDY OF THE AGING PRECIPITATION AND HARDENING BEHAVIOR OF 6005A ALLOY SHEET FOR RAIL TRAFFIC VEHICLE[J]. Acta Metall Sin, 2010, 46(12): 1481-1487.
| [1] Hirsch J. Mater Sci Forum, 1997; 242:33
[2] Miller W S, Zhuang L, Bottema J, Wittebrood A J, De Smet P, Haszler A, Vieregge A. Mat Sci Eng A-Struct,2000; 250(1):37
[3]Moons T, Ratchev P, De Smet P, Verlinden B, Van Houtte P. Scripta Mater, 1996; 35(8):937
[4] Birol Y. Eng Fail Anal, 2010; 17(5):1110
[5] Xiao C W, Wang M P, Wang Z A, Li Z, Guo M X. Chin J Nonferrous Met, 2003;13(3):635
(肖从文, 汪明朴, 王正安, 李周, 郭明星. 中国有色金属学报,2003;13(3):635)
[6] Buha J, Lumley R Crosky A G, Hono K. Acta Mater, 2007; 55(9):3015
[7] Yang C G, Shan J G, Xiong W. Welding & Joining, 2009; 10:13
(杨成功 ,单际国, 熊伟. 焊接, 2009; 10:13)
[8] Birol Y. Scripta Mater, 2005; 52(3):169
[9] Andersen S J. Metall Mater Trans A, 1995; 26:1931
[10] Zandergen H W, Andersen S J, Jansen J. Science, 1997; 277:1221
[11] Andersen S J, Zandergen H W, Jansen J, Tr?holt C, Tundal U, Reiso O. Acta Mater,1998; 46(9):3283
[12] Edwards G A, Stiller K, Dunlop G L, Couper M J.Acta Mater, 1998; 46(11):3893
[13] Chakrabarti D J,Yingguo P, Laughlin DE. Mater Sci Forum, 2002; 392:857
[14] Wang X, Esmaeili D, Lloyd D J. Metall Mater Trans A, 2006; 37:2691
[15] Marioara C D, Andersen S J, Zandbergen H W, Holmestad R. Metall Mater Trans A, 2005;36:691
[16] Murayama M, Hono K. Acta Mater, 1999; 47(5):1537
[17] Gaber A, Mossad A, Matsuda K, Kawabata T, Yamazaki T, Ikeno S. J Alloy Compd, 2007; 432:149
[18] Yassar R S, Field D P, Weiland H. Scripta Mater, 2005; 53: 299
[19] Matsuda K, Ikeno S, Matsui H, Sato T. Metall Mater Trans A, 2005; 36:2007
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|