| 氟离子注入纯Ti表面改性对成骨细胞I型胶原形成和表达的影响 |
| 刘慧颖1;2;王学金3;王浪平4;王小峰4;艾红军1 |
1.中国医科大学口腔医学院口腔修复科
2.大连医科大学口腔医学院口腔修复科
3.大连大学附属中山医院口腔科
4.哈尔滨工业大学现代焊接生产技术国家重点实验室 |
|
| INFLUENCE OF SURFACE MODIFICATION OF Ti BY FLUORINE ION-IMPLANTATION ON FORMATION AND EXPRESSION OF COLLAGEN-I ON OSTEOBLAST |
| LIU Huiying1;2;WANG Xuejin3;WANG Langping4;WANG Xiaofeng4;AI Hongjun1 |
1.Department of Prosthodontics; School of Stomatology; China Medical University
2.Department of Prosthodontics; School of Stomatology; Dalian Medical University
3.Department of Stomatology; Affiliated Zhongshan Hospital of Dalian University
4.State Key Laboratory of Advanced Welding Production Technology; Harbin Institute of Technology |
引用本文:
刘慧颖 王学金 王浪平 王小峰 艾红军. 氟离子注入纯Ti表面改性对成骨细胞I型胶原形成和表达的影响[J]. 金属学报, 2008, 44(12): 1485-1490.
,
,
,
,
.
INFLUENCE OF SURFACE MODIFICATION OF Ti BY FLUORINE ION-IMPLANTATION ON FORMATION AND EXPRESSION OF COLLAGEN-I ON OSTEOBLAST[J]. Acta Metall Sin, 2008, 44(12): 1485-1490.
[1]Kieswetter K,Schwartz Z,Dean D D,Boyan B D.Crit Rev Oral Biol Med,1996;7:329 [2]Zhu L,Ye X,Tang G,Zhao N,Gong Y,Zhao Y,Zhao J, Zhang X.J Biomed Mater Res,2006;78:515 [3]Mombelli A,Schmid B,Rutar A,Lang N P.J Clin Peri- odontol,2002;29:743 [4]Hemmings K W,Schmitt A,Zarb G A.Int J Oral Max- illofac Implants,1994;9:191 [5]Buser D,Ingimarsson S,Dula K,Lussi A,Hirt H P,Belser U C.Int J Periodontics Restorative Dent,2002;22:109 [6]Farley J R,Wergedal J E,Barlink D J.Science,1983;222: 330 [7]Kassem M,Mosekilde L,Eriksen E F.Eur J Endocrinol, 1994;130:381 [8]Reed B Y,Zerwekh J E,Antich P P,Pak C Y.J Bone Miner Res,1993;8:19 [9]Skartveit L,Selvig K A,Myklebust S,Tveit A B.Acta Odontol Scand,1990;48:169 [10]Yoshinari M,Oda Y,Kato T,Okuda K,Hirayama A.J Biomed Mater Res,2000;52:388 [11]Yoshinari M,Oda Y,Kato T,Okuda K.Biomaterials, 2001;22:2043 [12]Tang B Y,Wang L P,Wang X F,Gan K Y,Wang S Y. Nucl Technol,2002;25:690 (汤宝寅,王浪平,王小峰,甘孔银,王松雁.核技术,2002;25:6901 [13]Wang J,Huang N,Yang P,Leng Y X,Sun H,Liu Z Y, Chu P K.Biomaterials,2004;25:3163 [14]Wu S L,Chu P K,Liu X M,Chung C Y,Ho J P Y,Chu C L,Tjong S C,Yeung K W K,Lu W W,Cheung K M C,Luk K D K.J Biomed Mater Res,2006;79A:139 [15]Charles D,Alexander V N,Anna K V,Juanita W A, Cedric J R,John R R J.NIST X-ray Photoelectron Spec- troscopy Database,http://srdata.nist.gov/xps/index.htm [16]Christine M D,Joseph R,Jacques J V.Inorg Chem,1987; 26:1212 [17]Liu H Y,Wang X J,Wang L P,Lei F Y,Wang X F,Ai H J.Appl Surf Sci,2008;254:6305 [18]EI Sayegh T Y,Pilliar R M,McCulloch C A.J Biomed Mater Res,2002;61:482 [19]Schliephake H,Scharnweber D,Dard M,Rossler S,Sewing A,Meyer J,Hoogestraat D.Clin Oral Implants Res,2002; 13:312 [20]Cooper L F,Zhou Y,Takebe J,Guo J,Abron A,Holmen A,Ellingsen J E.Biomaterials,2006;27:926 |
|