| 金属玻璃中程有序结构的FEM技术表征 |
| 文军;王建强;马恩 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室 |
|
| A fluctuation electron microscopy study of metallic glasses |
| ;Jianqiang Wang;En Ma |
| 联合 |
引用本文:
文军; 王建强; 马恩 . 金属玻璃中程有序结构的FEM技术表征[J]. 金属学报, 2008, 44(11): 1388-1393 .
,
,
.
A fluctuation electron microscopy study of metallic glasses[J]. Acta Metall Sin, 2008, 44(11): 1388-1393 .
[1]Wang W H.Prog Mater Sci,2007;52:540 [2]Treacy M M J,Gibson J M.Acta Cryst,1996;52A:212 [3]Hufnagel T C.Nature Mater,2004;3:666 [4]Teacy M M J,Gibson J M,Fan L,Paterson D G,McNulty I.Rep Prog Phys,2005;68:2899 [5]Inoue A,Matsumoto N,Masumoto T.Mater Trans JIM, 1990;31:493 [6]Xu D H,Duan G,Johnson W L.Phys Rev Lett,2004;92: 245504 [7]Wang D,Tan H,Li Y.Acta Mater,2005;53:2969 [8]Yu P,Bai H Y,Tang M B,Wang W L.J Non-Cryst Solids, 2005;351:1328 [9]Kumar G,Ohkubo T,Mukai T,Hono K.Scr Mater,2007; 57:173 [10]Park K W,Jang J,Wakeda M,Shibutani Y,Lee J C.Scr Mater,2007;57:805 [11]Rudee M L,Howie A.Philo Mag,1972;25:1001 [12]Chaudhari P,Graczyk J F,Charbnau H P.Phys Rev Lett, 1972;29:425 [13]Voyles P M.PhD Dissertation,University of Illinois at Urbana-Champaign,Urbana,2000 [14]Wen J,Yang H W,Guo H,Wu B,Sui M L,Wang J Q, Ma E.J Phys:Condens Matter,2007;19:455211 [15]Stratton W G,Hamann J,Perepezko J H,Voyles P M, Mao X,Khare S V.Appl Phys Lett,2005;86:141910 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|