| 非化学计量比MnFe(P, Si, Ge)合金在低场下的磁热效应 |
| 王高峰;松林;李福安;哈斯朝鲁;李新文;特古斯 |
| 内蒙古师范大学 |
|
| Magnetocaloric effect on low field in non-stoichiometric MnFe(P,Si,Ge) alloys |
| Gao-Feng WANG;Lin SONG;;;; |
| 内蒙古师范大学 |
引用本文:
王高峰; 松林; 李福安; 哈斯朝鲁 ; 李新文; 特古斯 . 非化学计量比MnFe(P, Si, Ge)合金在低场下的磁热效应[J]. 金属学报, 2007, 43(8): 889-892 .
,
,
,
,
,
.
Magnetocaloric effect on low field in non-stoichiometric MnFe(P,Si,Ge) alloys[J]. Acta Metall Sin, 2007, 43(8): 889-892 .
[1]Tegus O,Brück E,Buschow K H J,de Boer F R.Nature, 2002;415:150 [2]Pecharsky V K,Gschneidner J K A.Phys Rev Lett,1997; 78:4494 [3]Brück E,Tegus O,Zhang L,Li X W,de Boer F R, Buschow K H J.J Alloys Compd,2004;383:32 [4]Tegus O,Fuquan B,Dagula W,Zhang L,Brück E,Si P Z,de Boer F R,Buschow K H J.J Alloys Compd,2005; 396:6 [5]Dagula W,Tegus O,Li X W,Song L,Brück E,Cam Thanh D T,de Boer F R,Buschow K H J.J Appl Phys, 2006;99:08Q105 [6]Brück E,Ilyn M,Tishin A M,Tegus O.J Magn Magn Mater,2005;290-291:8 [7]Tegus O,Brück E,Li X W,Zhang L,Dagula W,de Boer E R,Buschow K H J.J Magn Magn Mater,2004;272-2?6: 2389 [8]Tegus O,Brück E,Zhang L,Dagula W,Buschow K H J, de Boer F R.Physica,2002;319B:174 [9]Brück E,Tegus O,Li X W,de Boer F R,Buschow K H J.Physic.a,2003;327B:431 [10]Zener C.Phys Rev,1951;82:403 [11]Millis A J,Littlewood P B,Shraiman B I.Phys Rev Lett, 1995;74:5144 [12]Zhang L.PhD Dissertation,University of Amsterdam, 2005 [13]Bacmann M,Soubeyroux J L,Barrett R.J Magn Magn Mater,1994;134:59 [14]McGuire T R,Gupta A,Duncombe P R.J Appl Phys, 1996;79:4549 [15]Dionne G F.J Appl Phys,1996;79:172% |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|