| 高温合金GH4169(Inconel 718)中磷晶界偏聚特性的实验研究 |
| 郑 磊;徐庭栋;邓 群;司 红;董建新 |
| 钢铁研究总院 高温材料研究所 |
|
| Experimental study of the characteristic of grain-boundary P segregation in GH4169 |
| XU Ting-dong |
| 钢铁研究总院 高温材料研究所 |
引用本文:
郑磊; 徐庭栋; 邓群; 司红; 董建新 . 高温合金GH4169(Inconel 718)中磷晶界偏聚特性的实验研究[J]. 金属学报, 2007, 43(8): 893-896 .
,
,
,
,
.
Experimental study of the characteristic of grain-boundary P segregation in GH4169[J]. Acta Metall Sin, 2007, 43(8): 893-896 .
[1]Holt R T,Wallace W.Int Met Rev,1976;21:1 [2]Seah M P.Acta Metall,1980;28:955 [3]Bieber C G,Decker R F.Trans AIME,1961;221:629 [4]Was G S,Kruger R M.Acta Metell,1985;33:841 [5]Was G S,Sung J K,Angeliu T M.Metall Trans,1992; 23A:3343 [6]Ohtani H,Feng H C,McMahon C J Jr,Mulford R A. Metall Trans,1976;7A:87 [7]Ohtani H,Feng H C,McMahon C J Jr.Metall Trans, 1976;7A:1123 [8]Lawrence E D,MacDonald N C,Palmberg P W.Handbook of Auger Electron Spectroscopy.Minneapolis,Minnesota: Physical Electronics Industries Press,1983:310 [9]Huang X,Chaturvedi M C,Richards N L,Jackman J. Acta Mater,1997;45:3095 [10]Guttmann M,Dumoulin P,Tan-Tai N,Fontaine P.Cor- rosion,1981;37:416 [11]McLean D.Grain Boundaries in Metals.Oxford:Oxford University Press,1957:118 [12]Xu T D,Cheng B Y.Prog Mater Sci,2004;49:109 [13]Xu T D,Song S H.Acta Metall,1989;37:2499 [14]Xu T D,Song S H,Shi H Z,Gust W,Yuan Z X.Acta Metall Mater,1991;39:3119 [15]Aust K T,Hanneman R E,Niessen P,Westbrook J H. Acta Metall,1968;16:291 [16]Westbrook J H,Wood D L.Nature,1961;192:1280 [17]Williams T M,Stoneham A M,Harries D R.Metall Sci, 1976;10:14 [18]Karlsson L,Norden H.Acta Metall,1988;36:1 [19]Li Q F,Li L,Zheng L,Liu E B,Jin G,Yang S L.J Mater Sci,2004;39:6551 [20]Shinoda T,Nakamura T.Acta Metall,1981;29:1631 [21]Dong J X,Xie X S,Thompson R G.Metall Mater Trans, 2000;31A:2135 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|