| 有外加相存在时Al-Si合金枝晶微观组织数值模拟 |
| 李斌;许庆彦;柳百成 |
| 清华大学机械工程系 |
|
| Numerical simulation of dendrite microstructure for Al-Si alloy with additive phase |
| LI Bin; XU Qingyan; LIU Baicheng |
| Key Laboratory for Advanced Materials Processing Technology; Ministry of Education of China; Department of Mechanical Engineering; Tsinghua University; Beijing 100084 |
引用本文:
李斌; 许庆彦; 柳百成 . 有外加相存在时Al-Si合金枝晶微观组织数值模拟[J]. 金属学报, 2007, 43(3): 240-248 .
,
,
.
Numerical simulation of dendrite microstructure for Al-Si alloy with additive phase[J]. Acta Metall Sin, 2007, 43(3): 240-248 .
[1]Jung C K,Jung S W,Nam H W,Han K S.J Compos Mater,2003;37:503 [2]Li B,Xu Q Y,Li X D,Liu B C.Acta Metall Sin,2005; 41:1303 (李斌,许庆彦,李旭东,柳百成.金属学报.2005;12:1303) [3]Li B,Xu Q Y,Li X D,Liu B C.ISIJ Int,2006;46:241 [4]Li B,Xu Q Y,Li X D,Liu B C.Acta Metall Sin,2006; 42:875 (李斌,许庆彦,李旭东,柳百成.金属学报,2006;42:875) [5]Nastac L.Acta Mater,1999;47:4253 [6]Zhu M F,Hong C P.ISIJ Int,2001;41:436 [7]Zhu M F,Hong C P.Metall Mater Trans,2004;35A:1555 [8]Beltran-Sanchez L,Stefanescu D M.Metall Mater Trans, 2003;34A:367 [9]Li Q,Li D Z,Qian B N.Acta Metall Sin,2004;40:634 (李强,李殿中,钱百年.金属学报.2004;40:634) [10]Kim J K,Rohatgi P K.Acta Mater,1998;46:1115 [11]Kim J K,Rohatgi P K.Metall Mater Trans,1998;29A: 351 [12]Stefanescu D M,Juretzko F R,Dhindaw B K,Catalina A V,Sen S,Curreri P A.Metall Mater Trans,1998;29A: 1697 [13]Catalina A V,Mukherjee S,Stefanescu D M.Metall Mater Trans,2000;31A:2559 [14]Dilthey U,Pavlik V.In:Thomas B G,Beckermann C,ed.,Proc 8th Int Conf on Modeling of Casting and Welding Processes,Warrendale,PA:TMS,1998:589 [15]Sasikumar R,Sreenivisan R.Acta Mater,1994;42:2381 [16]Stefanescu D M,Dhindaw B K,Kacar S A,Moitra A. Metall Mater Trans,1988;19A:2847 [17]Sekhar J A,Trivedi R.In:Rohatgi P K,ed.,Solidifica- tion of Metal Matrix Composites,Warrendale,PA:TMS, 1990:39 [18]Kim J K,Rohatgi P K.Metall Mater Trans,2000;31A: 1295 [19]Juretzko F R,Dhindaw B K,Stefanescu D M,Sen S,Cur- ??reri P A.Metall Mater Trans,1998;29A:1691 [20]Omenyi S N,Neumann A W.J Appl Phys,1976;47:3956 [21]Garvin J W,Udaykumar H S,J Cryst Growth,2003;252: 451 [22]Wu Y,Liu H,Lavernia E J.Acta Metall Mater,1994;42: 825 [23]Shangguan D,Ahuja S,Stefanescu D M.Metall Mater Troths,1992;23A:669 [24]Feng W M.Master Degree Thesis,Tsinghua University, Beijing,2002:66 (冯伟明.清华大学硕士学位论文,北京,2002:66) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|