| 铝合金压铸过程铸件/铸型界面换热行为的研究I. 实验研究和界面换热系数求解 |
| 郭志鹏 熊守美 曺尚铉 崔正吉 |
| 清华大学机械工程系清华--东洋镁铝合金成形技术研究开发中心 |
|
引用本文:
郭志鹏; 熊守美; 曺尚铉; 崔正吉 . 铝合金压铸过程铸件/铸型界面换热行为的研究I. 实验研究和界面换热系数求解[J]. 金属学报, 2007, 43(11): 1149-1154 .
[1]Li M,Zindel J,Godlewski L,Allison J.TMS Lett,2006; (2):31 [2]Dour G,Dargusch M,Davidson C,Nef A.J Mater Process Technol,2005;169:223 [3]Griffiths W D.Metall Mater Trans,2000;31B:285 [4]Hallam C P,Griffiths W D.Metall Mater Trans,2004; 35B:721 [5]Guther R I L,Isac M,Kim J S,Tavares R P.Metall Mater Trans,2000;31B:1031 [6]Hines J A.Metall Mater Trans,2004;35B:299 [7]Michalski L,Echersdort K,McGhee J.Temperature Mea- surement.New York:Wiley,1991:220 [8]Beck J V,Blackwell B,Clair C R S T.Inverse Heat Con- duction.Ill-posed Problems.New York:Wiley,1985:145 [9]Keith A,Woodbury A.Int J Heat Mass Trans,1990;33: 2641 [10]Guo Z P,Xiong S M,Cho S H,Choi J K.Acta Metall Sin, 2007;43 :103 (郭志鹏,熊守美,曺尚铉,崔正吉.金属学报,2007;43:103) [11]Ho K,Pehlke R D.Metall Trans,1985;16B:585 [12]Santos C A,Quaresma J M V,Garcia A.J Alloys Compd, 2001;319:179 [13]Michel F,Louchez P R,Samuel F H.Trans AFS,1995; 103:275 [14]Prabhu K N,Kumar S A,Venkataraman N.Trans AFS, 1994;102:827 [15]Lau F,Lee W B,Xiong S M,Liu B C.J Mater Process Technol,1998;79:25 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|