| 过冷 Fe75Ni25合金晶粒细化机制的研究 |
| 陈豫增 杨根仓 刘 峰 刘 宁 谢 辉 周尧和 |
| 西北工业大学凝固技术国家重点实验室; 西安 710072 |
|
| Research on Grain Refinement Mechanism in Undercooled Fe75Ni25 Alloy |
| CHEN Yuzeng; YANG Gencang;LI Feng; LIU Ning; XIE Hui; ZHOU Yaohe |
| State Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi'an 710072 |
引用本文:
陈豫增; 杨根仓; 刘峰; 刘宁; 谢辉; 周尧和 . 过冷 Fe75Ni25合金晶粒细化机制的研究[J]. 金属学报, 2006, 42(7): 703-707 .
,
,
,
,
,
.
Research on Grain Refinement Mechanism in Undercooled Fe75Ni25 Alloy[J]. Acta Metall Sin, 2006, 42(7): 703-707 .
[1] Herlach D M.Mater Sci Eng, 1994; R12: 177 [2] Walker J L.In: Pierre G L St,ed.,The Physical Chemistry of Process Metallurgy(Part 2),NY:Interscience, 1959: 845 [3] Li J F, Yang G C, Zhou Y H.Mater Res Bull,1998; 33: 141 [4] Dragnevski K I,Cochrane R F, Mullis A M. Mater Sci Eng, 2004; A375-377: 479 [5] Schwarz M,Karma A,Eckler K,Herlach D M.Phys Rev Lett, 1994; 73: 1380 [6] Liu Fe, Yang G C, Guo X F. Mater Sci Eng, 2001; A311:54 [7] Li J F, Liu Y C, Lu Y L, Yang G C, Zhou Y H. J Cryst Growth, 1998; 192: 462 [8] Eckler K, Norman A F, Gartner F, Greer A L, Herlach D M. J Cryst Growth, 1997; 173: 528 [9] Liu N, Yang G C, Chen Y Z, Zhou Y H. Prog Nat Sci,2006; 16(1): 120 (刘宁,杨根仓,陈豫增,周尧和,自然科学进展,2006;16(1): 120) [10] Jackson K A, Hunt J D, Uhlmann D R, Stewart T P.TMS-AIME, 1966; 236: 149 [11] Horvay G. Int J Heat Mass Transfer, 1965; 8: 195 [12] Kobayashi K F, Hogan L M. Met Forum, 1978; 1: 165 [13] Karma A. Int J Non-Equilib Process, 1998; 11: 201 [14] Mullis A M, Cochrane R F. J Appl Phys, 1997; 82: 1380 [15] Herlach D M, Eckler K, Karma A, Schwarz M. Mater Sci Eng, 2001; A304-306: 20 [16] Zambon A,Badan B,Eckler K, Gartner F,Norman A F,Greer A L,Herlach D M,Ramous E. Acta Mater,1998;46: 4657 [17] Chuang Y Y and Chang Y A. Met Trans, 1987; 18A: 733 [18] Chen Y Z, Yang G C, Liu F, Liu N, Xie H, Zhou Y H. J Cryst Growth, 2005; 282: 490 [19] Boettinger W J,Coriell S R,Trivedi R. In: Mehrabian R,Parrish P A, eds., Rapid Solidification Processing:Principles and Technologies IV, Baton Rouge, LA: Claitor's Pulishing Division,1988: 13 [20] Branders E A.Smithells Metals Reference Book. 6th ed.,London: Butterworths,1991 [21] Piccone T J, Wu Y, Shiohara Y, Flemings M C. Metall Trans, 1987; 18A: 925 [22] Aziz M J. J Appl Phys, 1982; 53: 1154 [23] Willnecker R, Herlach D M, Feuerbacher B. Appl Phys Lett, 1990; 56: 324 [24] Barth B, Eckler K, Herlach D M, Alexander H. Mater Sci Eng, 1991; A133: 790 [25] Powell G L F. TMS-AIME, 1969; 245: 1785O |
|