| 退火及置换元素对Fe-Cr-Al基合金阻尼性能及强度的影响 |
| 林仁荣 刘 芳 曹名洲 杨 锐 |
| 中国科学院金属研究所;沈阳 110016 |
|
| INFLUENCE OF ANNEALING AND SUBSTITUTION ELEMENTS ON DAMPING CAPACITY AND STRENGTH OF Fe-Cr-Al BASED ALLOYS |
| LIN Renrong; LIU Fang; CAO Mingzhou; YANG Rui |
| Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
林仁荣; 刘芳; 曹名洲; 杨锐 . 退火及置换元素对Fe-Cr-Al基合金阻尼性能及强度的影响[J]. 金属学报, 2005, 41(9): 958-962 .
,
,
,
.
INFLUENCE OF ANNEALING AND SUBSTITUTION ELEMENTS ON DAMPING CAPACITY AND STRENGTH OF Fe-Cr-Al BASED ALLOYS[J]. Acta Metall Sin, 2005, 41(9): 958-962 .
[1] Zheng W J, Lu J S, Zhang J, Wu B R. J Iron Steel Res, 1997; 9(1): 17 (郑文杰,陆军生,张杰,吴宝榕.钢铁研究学报,1997;9(1): 17) [2] Zhang J X. Dev Appl Mater, 1991; 6(2): 2 (张俊旭.材料开发与应用,1991;6(2):2) [3] Azcoitia C, Karimi A. J Alloys Compd, 2000; 310: 160 [4] Karimi A, Azcoitia C, Degauque J. J Magn Magn Mater, 2000; 215-216: 601 [5] Cochardt A W. J Appl Phys, 1954; 25: 670 [6] Lin R R, Cao M Z, Yang R. Mater Sci Forum, 2005; 475- 479: 261 [7] Lavernia E J, Perez R J, Zhang J. Metall Mater Trans, 1995; 26A: 2803 [8] Smith G W, Birchak J R. J Appl Phys,1968;39: 2311 [9] Smith G W, Birchak J R. J Appl Phys,1969;40:5174 [10] Zener C. Elasticity and Anelasticity of Metals.Chicago: University of Chicago Press,1948: 64 [11] Wang W G, Mo D X,Zhao T T, Zhang Y.J Shandong Inst Technol, 2002; 16(1): 23 (王卫国,莫德秀,赵婷婷,张勇.山东工程学院学报,2002; 16(1):23) [12] Wang W G, Liu S G, Xue B. J Shandong Inst Technol, 2002; 16(4): 41 (王卫国,刘曙光,薛冰.山东工程学院学报,2002;16(4): 41) [13] Ha K F. Microscopic Theory of Metallic Mechanical Properties. Beijing: Science Press, 1983: 350 (哈宽富.金属力学性质的微观理论.北京:科学出版社,1983: 350) |
|