| 用XD法合成的铝基复合材料的组织与力学性能 |
| 朱和国 王恒志 熊党生 吴申庆 |
| (南京理工大学材料科学与工程系; 南京 210094) |
|
引用本文:
朱和国; 王恒志; 熊党生; 吴申庆 . 用XD法合成的铝基复合材料的组织与力学性能[J]. 金属学报, 2005, 41(8): 829-834 .
[1] Michal B, Jozef I, Ladislav K. Mater Lett, 2000; 46: 181 [2] Tsang H, Chao C G, Ma C Y. Scr Mater, 1997; 37: 1359 [3] Ma Z Y, Lu Y X, Bi J. Ada Metall Sin, 1999; 35: 98 (马宗义,吕毓雄,毕 敬.金属学报, 1999;35:98) [4] Chen J, Wang Z F, Bian J H, Wang X M. Acta Metall Sin, 2001; 37: 207 (陈俊,王执福,边建华,王晓明.金属学报,2001;37:207) [5] Tjong S G, Ma Z Y. Mater Sci Eng, R-Report. 2000; 29: 49 [6] Lv W J, Zhang D, Zhang X N, Wu R J, Sakata T, Mori H. Mater Sci Eng, 2001; A311: 142 [7] Peng H X, Fan Z, Wang D Z. J Mater Res, 2000; 15: 1943 [8] Yang B, Zhang E L, Zeng S Y, Dai S L, Liu B C. Chin J Nonferrous Met, 2001; 11: 846 (杨 波,张二林,曾松岩,戴圣龙,刘伯操.中国有色金属学 报,2001;11:846) [9] Zhu H G. PhD Dissertation, Southeast University, Nanjing, 2003 (朱和国.东南大学博士学位论文,南京, 2003) [10] Ma Z Y, Li J H, Li S X, Ning X G, Lv Y X, Bi J. J Mater Sci, 1996; 31: 741 [11] Wu S Q, Zhu II G, Tjong S G. Metall Mater Trans, 1999; 30A: 243 [12] Zhu H G, Wang H Z, Wu S Q. Acta Metall Sin, 2002; 38: 385 (朱和国,王恒志,吴申庆.金属学报,2002;38:385) [13] Yu H S, Min W H, Chen X C. Acta Mater Compos Sin, 2000; 17(3): 113 (于化顺,闵文辉,陈熙琛.复合材料学报,2000;17(3):113) [14] Garcia E, Janssen R. J Mater Sci, 1999; 34: 769 [15] Schumacher P, Greer A L. In: Evans J ed., Light Met, Warrendale, PA: TMS, 1995: 869 [16] Edit Group of the Metal Mechanical Property. Metal Mechanical Property. Beijing: China Machine Press, 1982: 71 (金属机械性能编写组.金属机械性能.北京:机械工业出版社, 1982:71) [17] Eston M, Stjohn D. Metall Mater Trans, 1999; 30A: 1613 [18] Clyne T W, Withers P J. An Introduction to Metal Matrix Composites, London: Cambridge University Press, 1993: 85 [19] Petch N J. J Iron Steel Inst, 1953; 25: 174 [20] Jiang C H, Wang D Z, Yao Z K. Acta Metall Sin, 2000; 36: 555 (姜传海,王德尊,姚忠凯.金属学报, 2000;36:555)P |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|