Please wait a minute...
金属学报  2005, Vol. 41 Issue (11): 1221-1227     
  论文 本期目录 | 过刊浏览 |
一种性能优异的过热器管材用高温合金GH2984
郭建亭; 杜秀魁
中国科学院金属研究所
A superheater tube superalloy GH2984 with excellent properties
GUO Jianting; DU Xiukui
Institute of Metal Research; The Chinese Academy of Sciences
引用本文:

郭建亭; 杜秀魁 . 一种性能优异的过热器管材用高温合金GH2984[J]. 金属学报, 2005, 41(11): 1221-1227 .
, . A superheater tube superalloy GH2984 with excellent properties[J]. Acta Metall Sin, 2005, 41(11): 1221-1227 .

全文: PDF(549 KB)  
摘要: 简要介绍一种性能优异的过热器管材用铁基高温合金GH2984的成分设计与性能. 该合金的特点是不含贵重元素Co, 且有32%-34% 的Fe, 因而成本低廉。分析了这一合金制作舰船用和超级超临界发电锅炉用过热器的优越性. 舰船实际应用结果表明, GH2984合金是一种性能优异的舰船用过热器管材合金. 该合金也是超级超临界燃煤电站锅炉用过热器和再热器管材用钢的重要候选材料.
关键词 : 铁基高温合金,  过热器材料,  力学性能    
Abstract:A superheater tube superalloy GH2984 with excellent properties had been successfully developed, which does not contains expensive element Co but has 32%-36% Fe, so it has low cost. In this paper, the characteristics of GH2984, including the chemical composition, mechanical and chemical properties, the microstructure stability after long-time thermal exposure and the processing property at hot and cold conditions have been introduced briefly. Then the superiority of this alloy used in ship boiler and ultra-supercritical coal-fired boiler as superheater was analyzed. The results from practical application to the ship boilers show that the GH2984 superalloy is suitable to the ship boiler superheater tube material, and the alloy also is very important candidate of a superheater and reheater materials in the ultra-supercritical steam boilers
Key words: Fe base superalloy    superheater material    mechanical property
收稿日期: 2005-06-30     
ZTFLH:  TG132.3  
[1] Institute of Metal Research, CAS, Shanghai No.5 Steel Plant, Harbin 703 Institute. The Investigation of GH2984 Superalloy, 1991 (中国科学院金属研究所,冶金工业部上海第五钢铁厂,造船总 公司七院703所. GH984合金研制总结,1991)
[2] Chen M, Ma Y X, Xue G Y, Chen Q D. Design Characteristic of Main Boiler in Certain Ship, 2004 (陈明,马玉翔,薛光亚,陈起铎.某船主锅炉的设计特点, 待发表资料,2004年)
[3] Lu Y S. Power Eng, 2003; 23: 2615 (陆燕荪.动力工程,2003;23:2615)
[4] Wang S H, Du X K, Xu H Z, Yu C S, Guo J T, Hu Q W. Acta Metall Sin, 1995; 31(Suppl.): S137 (王淑荷,杜秀魁,许惠珍,于长生,郭建亭,胡秋文.金属学 报,1995;31(增刊):S137)
[5] Wang S H, Du X K, Guo J T. Trans Met Heat Treat, 1998; 19(3):36 (王淑荷,杜秀魁,郭建亭.金属热处理学报,1998;19(3):36)
[6] Wang S H, Du X K, Zhao J F, Guo J T. Mater Mech Eng, 1999; 23(2): 34 (王淑荷,杜秀魁,赵金福,郭建亭.机械工程材料,1999;23(2): 341
[7] Wang S H, Du X K, Guo J T, Xu H Z. Corros Sci Prot Technol, 2002; 14: 284 (王淑荷,杜秀魁,郭建亭,许惠珍.腐蚀科学与防护技术,2002; 14:284)
[8] Wang S H, Du X K, Xu H Z, Guo J T, Hu Q W. Trans Met Heat Treat, 1995; 16(3): 51 (王淑荷,杜秀魁,许惠珍,郭建亭,胡秋文.金属热处理学报, 1995;16(3):51)
[9] Zhao S Q, Dong J X, Zhang M C, Xie X S. J Iron Steel Res, 2003; 15(7): 160 (赵双群,董建新,张麦仓,谢锡善.钢铁研究学报,2003;15(7): 160)
[10] Institute of Metal Research, CAS. Mechanical Properties and Microstructure Stability of GH2984 Superalloy after Long-time Thermal Exposure at 700℃, 1991 (中国科学院金属研究所. GH2984合金700℃长期时效后的 性能和组织稳定性的研究, 1991)
[11] Stroh A N. Proc R Soc London, 1954; 223A: 404
[12] Zhao G P, Zhao B K. In: China Aeronautical Materials Handbook, Vol.2, Beijing: China Standard Press, 2002:399 (赵光普,赵炳堃.见:中国航空材料手册编辑委员会编,中国 航空材料手册,第2卷.北京:中国标准出版社,2002:399)
[13] Zhao S Q, Dong J X, Xie X S, Smith G D, Patel S J. In: Green K A, Pollock T M, Harada H. eds., Superalloy 2004, Champion, PA: TMS, 2004: 63
[1] 郑亮, 张强, 李周, 张国庆. 增/降氧过程对高温合金粉末表面特性和合金性能的影响:粉末存储到脱气处理[J]. 金属学报, 2023, 59(9): 1265-1278.
[2] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[3] 张健, 王莉, 谢光, 王栋, 申健, 卢玉章, 黄亚奇, 李亚微. 镍基单晶高温合金的研发进展[J]. 金属学报, 2023, 59(9): 1109-1124.
[4] 张雷雷, 陈晶阳, 汤鑫, 肖程波, 张明军, 杨卿. K439B铸造高温合金800℃长期时效组织与性能演变[J]. 金属学报, 2023, 59(9): 1253-1264.
[5] 李景仁, 谢东升, 张栋栋, 谢红波, 潘虎成, 任玉平, 秦高梧. 新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理[J]. 金属学报, 2023, 59(8): 1087-1096.
[6] 陈礼清, 李兴, 赵阳, 王帅, 冯阳. 结构功能一体化高锰减振钢研究发展概况[J]. 金属学报, 2023, 59(8): 1015-1026.
[7] 丁桦, 张宇, 蔡明晖, 唐正友. 奥氏体基Fe-Mn-Al-C轻质钢的研究进展[J]. 金属学报, 2023, 59(8): 1027-1041.
[8] 袁江淮, 王振玉, 马冠水, 周广学, 程晓英, 汪爱英. Cr2AlC涂层相结构演变对力学性能的影响[J]. 金属学报, 2023, 59(7): 961-968.
[9] 吴东江, 刘德华, 张子傲, 张逸伦, 牛方勇, 马广义. 电弧增材制造2024铝合金的微观组织与力学性能[J]. 金属学报, 2023, 59(6): 767-776.
[10] 侯娟, 代斌斌, 闵师领, 刘慧, 蒋梦蕾, 杨帆. 尺寸设计对选区激光熔化304L不锈钢显微组织与性能的影响[J]. 金属学报, 2023, 59(5): 623-635.
[11] 张东阳, 张钧, 李述军, 任德春, 马英杰, 杨锐. 热处理对选区激光熔化Ti55531合金多孔材料力学性能的影响[J]. 金属学报, 2023, 59(5): 647-656.
[12] 刘满平, 薛周磊, 彭振, 陈昱林, 丁立鹏, 贾志宏. 后时效对超细晶6061铝合金微观结构与力学性能的影响[J]. 金属学报, 2023, 59(5): 657-667.
[13] 李述军, 侯文韬, 郝玉琳, 杨锐. 3D打印医用钛合金多孔材料力学性能研究进展[J]. 金属学报, 2023, 59(4): 478-488.
[14] 吴欣强, 戎利建, 谭季波, 陈胜虎, 胡小锋, 张洋鹏, 张兹瑜. 耐Pb-Bi腐蚀Si增强型铁素体/马氏体钢和奥氏体不锈钢的研究进展[J]. 金属学报, 2023, 59(4): 502-512.
[15] 唐伟能, 莫宁, 侯娟. 增材制造镁合金技术现状与研究进展[J]. 金属学报, 2023, 59(2): 205-225.