| 含Ca, Si镁合金的铸态组织及其形成机制 |
| 艾延龄 罗承萍 刘江文 黄雁飞 |
| 华南理工大学机械工程学院; 广州 510641 |
|
| As--Cast Microstructure and its Formation Mechanism in Mg-Based Alloys Containing Ca And Si |
| AI Yanling; LUO Chengping; LIU Jiangwen; HUANG Yanfei |
| College of Mechanical Engineering; South China University of Technology; Guangzhou 510641 |
引用本文:
艾延龄; 罗承萍; 刘江文; 黄雁飞 . 含Ca, Si镁合金的铸态组织及其形成机制[J]. 金属学报, 2005, 41(1): 49-.
,
,
,
.
As--Cast Microstructure and its Formation Mechanism in Mg-Based Alloys Containing Ca And Si[J]. Acta Metall Sin, 2005, 41(1): 49-.
[1] Mordike B L, Ebert T. Mater Sci Eng, 2001; A302: 37 [2] Carbonneau Y, Couture A, van Neste A, Tremblay R. Metall Mater Trans, 1998; 29A: 1759 [3] You B S, Park W W, Chung I S. Scr Mater, 2000; 42:1089 [4] Kim J J, Kim D H, Skin K S , Kim N J. Scr Mater, 1999;41: 333 [5] Yuan G Y, Liu Z L, Wang Q D, Ding W J. Mater Lett,2002; 56: 53 [6] Yuan G Y, Liu M P, Ding W J, Akihisa I. Mater Sci Eng,2003; A357: 314 [7] Nie J F, Muddle B C. Scr Mater, 1997; 37: 1475 [8] Bronfin B, Katsir M, Aghion E. Mater Sci Eng, 2001;A302: 46 [9] Villars P, Prince A, Okumoto H. Handbook of TernaryAlloy Phase Diagram. ASM International, 1995: 66 [10] Matsui H, Kuramoto M, Ono T, Nose Y, Tatsuoka H, Ki-wabara H. J Cryst Growth, 2002; 237-239: 2121 [11] Hosono J, Kuramoto M. Appl Surf Sci, 2003; 216: 620 [12] Luo C P, Weatherly G C. Acta Metall, 1963; 35: 1987 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|