| Gasar工艺中金属-氢二元相图的研究 |
| 张华伟 李言祥 刘 源 |
| 清华大学机械工程系; 北京 100084 |
|
| Study of Metal--Hydrogen Binary Phase Diagram in Gasar Process |
| ZHANG Huawei; LI Yanxiang; LIU Yuan |
| Department of Mechanical Engineering; Tsinghua University; Beijing 100084 |
引用本文:
张华伟; 李言祥; 刘源 . Gasar工艺中金属-氢二元相图的研究[J]. 金属学报, 2005, 41(1): 55-.
,
,
.
Study of Metal--Hydrogen Binary Phase Diagram in Gasar Process[J]. Acta Metall Sin, 2005, 41(1): 55-.
[1] Shapovalov V I. US Pat, No. 5, 181, 549. January 26, 1993 [2] Walukas D M. GASAR Materials: A Novel Approach inthe Fabrication of Porous Materials. DMK TEK INC.,Ann Arbor, MI, 1992-1 [3] Shapovalov V I. MRS Bull, 1994; 19(4): 24 [4] http://www.mrs.org/meetings/spring98/progbook/ProgramBookR.htmlhttp://www.mrs.org/meetings/spring94/progbook/ProgramBookR.html [5] Zheng Y, Sridhar S, Russell K C. Mater Res Soc SympProc, 1995; 371. 365 [6] Yu Z. MSC Thesis, USA: MIT, 1995; 1:46 [7] Yu J Q, Yi W Z, Chen B D, Chen H J. Collective Draw-ings of Binary Alloy State Diagram. Shanghai: ShanghaiScience and Technology Press, 1987: 6(虞觉奇,易文质,陈邦迪,陈宏鉴.二元合金状态图集 上海:上海科学技术出版社, 1987:6) [8] Smithells C J. Metals Reference Book (Fifth Edition).London: Butterworth & Co., Ltd., 1976: 231 [9] Vol A E.Handbook of Binary Metallic Systems. Jerusalem:Israel Program for Scientific Translations, 1967; 2: 290 [10] Sridhar S. MSC Thesis, Sweden: Royal Institute of Tech-nology, 1994: 73 [11] Shapovalov V I, Semik A P, Timchenko A G. Metallurgy, 1993; (3) 25j |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|