| 初生硅在熔体中的溶解动力学 |
| 张蓉 赵志龙 刘汉武 刘林 |
| 西北工业大学应用物理系;西安710072 |
|
引用本文:
张蓉; 赵志龙; 刘汉武; 刘林 . 初生硅在熔体中的溶解动力学[J]. 金属学报, 2002, 38(4): 397-399 .
[1] Tien J K, Gamble R P. Mater Sci Eng,1971; 8: 152 [2] Bhambri A K, Kattamis T Z, Morral E. Metall Trans,1975; 6B: 523 [3] Fernandez R, Lecomte J C, Kattamis T Z. Metall Trans,1978; 9A: 1381 [4] Wan X, Han Q, Hunt J D. Metall Mater Trans, 1998; 29A:751 [5] Wang R Y, Lu W H, Hogon L M. Mater Sci Technol, 1995;11: 441 [6] Yilmaz F, Atasoy O A. J Cryst Growth, 1992; 118: 377 [7] Aaron H B, Kotler G R. Met Sci J, 1970; 4: 222 [8] Aaron H B, Kotler G R. Metall Trans, 1971; 2: 393 [9] Min N B. The Physical Principle of Crystal Growth.Shanghai: Shanghai Science and Technology Press, 1982:305(闵乃本.晶体生长的物理基础.上海:上海科学技术出版社,1982:305) [10] Cheney W, Kincaid D. Translated by Xue M. NumericalMathematics and Computing. Shanghai: Fudan Univer-sity Press. 1991: 350(Cheney W,Kincaid D著,薛 密译.数值数学和计算.上海:复旦大学出版社.1991:350) [11] Tao W M. Mater Sci Eng, 1988: 6(4): 16(陶为民 材料科学与工程,1988;6(4):16) [12] Gunduz M, Hunt J D. Acta Metall, 1985; 33: 1651 [13] Zhang R, Geng X G, Wang L D, Xiong Y H, Zhang Y W,Liu L. J Aeronautic Maten 1995; 15: 39(张 蓉,耿兴国,王六定,熊玉华,张元雯,刘 林.航空材料学报,1995;15:39) [14] Zhang R. PhD Thesis, Northwestern Polytechnical Uni-versity xi'an. 2000 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|