| 电磁铸造对2024铝合金力学性能和组织的影响 |
| 贾非 金俊泽 曹志强 张兴国 郝海 |
| 大连理工大学铸造工程研究中心;大连116024 |
|
引用本文:
贾非; 金俊泽; 曹志强; 张兴国; 郝海 . 电磁铸造对2024铝合金力学性能和组织的影响[J]. 金属学报, 2002, 38(4): 393-396 .
[1] Getselev Z N. J Met, 1971; 23(10): 38 [2] Prasso D C, Evans J W, Wilson I J. Metall Trans, 1995;26B: 1243 [3] Furui M, Kojima Y, Matsuo M. ISIJ Int, 1993; 33: 400 [4] Polmear I J. Light Alloys. London: Edward Arnold, 1995:58 [5] Zhang B, Poirier D R, Chen W. Metall Mater Trans, 1999;30A: 2659 [6] Jiang H, Brown P, Knott J F. J Mater Sci, 1999; 34: 719 [7] Ricou R, Vives C. Metall trans, 1985; 16B: 377 [8] Sakane J, Li B Q, Evans J W. Metall Trans, 1988; 19B:397 [9] Jiang X J, Noble B, Holme B, Waterloo G, Tafto J. MetallMater Trans, 2000; 31A: 339 [10] Higgins R A. The Properties of Engineering Materials.London: Edward Arnold, 1994: 264 [11] Yuan S Y, Yeh J W, Tsau C H. Mater Trans JIM 1999;40: 233 [12] Miao W F, Laughlin D E. J Mater Sci Lett, 2000; 19: 201g |
|