| AZ91合金的热裂行为研究 |
| 王业双 丁文江 王渠东 朱燕萍 |
| 上海交通大学轻合金精密成形国家工程研究中心;上海200030 |
|
引用本文:
王业双; 丁文江; 王渠东; 朱燕萍 . AZ91合金的热裂行为研究[J]. 金属学报, 2001, 37(5): 527-530 .
[1] Luo A, Pekguleryuz M O. J Mater Sci, 1994; 29: 5259 [2] Warrington D, McCartney D G. Cast Met, 1989; (2): 134 [3] Wang Y S, Ding W J, Wang Q D. Spec Cast NonferrousAlloys, 2000; (2): 48 (王业双,丁文江,王渠东.特种铸造及有色合金,2000;(2):48) [4] Sigworth G K. AFS Trans, 1996; (155): 1053 [5] American Society for Metals. Metals Handbook, NinthEdition, Volume 2. Beijing: Mechanical Industry Press,1994: 751 (美国金属学会编.金属手册.第九版,第二卷,北京:机械工业出版,1994:751 [6] Yuan G Y. Ph D Dissertation, Southeast University, 1999 (袁广银.东南大学博士学位论文,1999) [7] Humble P. Mater Forum, 1997; 21: 45 [8] Chinese Mechanical Engineering Academy ed. FoundryMan, Vol 3, Beijing: Engineering Industry Press, 1993: 7 (中国机械工程学会编.铸造手册.北京:机械工业出版社,1993 [9] Li Q C. Mechanism of Casting Formation. Beijing: Engineering Industry Press,1982:118 (李庆春.铸件形成理论基础.北京:机械工业出版社,1982:118) [10] Kim K, Han H N, Yeo T, Lee Y, Oh K H, Lee D N. Ironmaking Steelmaking, 1997; 24: 249( |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|