| Zr-4合金双轴疲劳行为及其微观变形机理Ⅱ.双轴循环变形亚结构及其?… |
| 肖林 白菊丽 |
| 西安交通大学金属材料强度国家重点实验室; 西安 710049 |
|
引用本文:
肖林; 白菊丽 . Zr-4合金双轴疲劳行为及其微观变形机理Ⅱ.双轴循环变形亚结构及其?…[J]. 金属学报, 2000, 36(9): 919-925 .
[1] Donng S H, Socie D F, Robertson I M. ASME J Eng MaterTechnol, 1990; 112: 456 [2] Doquet V, Pineau A. Scripta Metall Mater,1990; 24: 433 [3] McDowell D L, Stahl S R, Stock S R, Antolovich S D.Metall Trans, 1988; 19A: 1277 [4] Nishino S, Hamada N, Sakane M, Ohnami M, MatsumuraN, Tokizane M. Fatigue Fract Eng Mater Struct, 1986; 9:65 [5] Kida S, Itch T, Sakane M, Ohnami M, Socie D F. FatigueFract Eng Mater Struct, 1997; 20: 1375 [6] Jiao F, Osterle W, Portella P D, Ziebs J. Mater Set Eng,1995; 196A: 19 [7] Ranch B F, Schmitt J H. Mat Sci Eng, 1989; All3: 441 [8] Thuillier S, Ranch E F. Acta Metall Mated 1994; 42: 1973 [9] Kanazawa K, Miller K J, Brown M W. Fatigue Fract EggMater Struct,1978; 2: 217 [10] Krempl E, Lu H. ASME J Eng Mater Technol, 1984; 106:376 [11] Benallal A, Marquis D. Trans ASME, 1987; 109: 326 [12] Feaugas X, Clavel M. Acta Mater,1997; 45: 2685 [13] Feaugas X, Pilvin P H, Clavel M. Acta Matal 1997: 45:2703 [14] Xiao L. ASME J Eng Mater Technol,2000; 120: 42 [15] Xiao L, Gu H C. Mater Sci Eng, 1998; 252. 166 [16] Xiao L, Gu H C. Metall Mater Trans, 1997; 28A: 1021 [17] Yoo M H. Metall Trans,1981; 12A: 409 [18] Xiao L, Gu H C. ASME J Eng Mater Technol, 1998; 120:114 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|