| 热处理对莫来石短纤维增强ZL107合金高温循环蠕变行为的影响 |
| 王珊玲 于维成 |
| 四川大学金属系; 成都 610065 |
|
引用本文:
王珊玲; 于维成 . 热处理对莫来石短纤维增强ZL107合金高温循环蠕变行为的影响[J]. 金属学报, 2000, 36(5): 550-554 .
[1]Fan J Z K,Li Y C.Mater Rev,1997;11(3):48 (樊建中,姚忠凯,李义春.材料导报,1997;11(3):48) [2] Cade K J,Pahutova M.Mater Sci Eng,1994;A20(1):141 [3] Li Y, Mohamed F A.Acta Mater,1997;45(11): 4775 [4] Liu P L,Wang G Z,Wang W L,Toda H,Kobayashi T.Acta Metall Sin, 1997; 33(11): 1227(刘丕林,王光中,王文龙,户田裕之,小林俊郎.金属学报,1997;33(11:1227) [5] Dlouhy A, Merk N, Eggeler G. Acta Metall Mater,1993;41:3245 [6] Krajewski P E,Allison J E,Jones J W.Metall Trans,1993; A24:2731 [7] Nardone V C, Kimmerle W L, Tien J K. Metall Trans1986;A17: 1577 [8] Stefani J A, Nardone V C, Tien J K. Scr Metall, 1987; 21:1 [9] Liu P L, Wang G Z, Wang W L. Mater Sci Tech, 1997;13: 667 [10] Liu P L, Wang G Z, Toda H,Kobayashi T. Scr Metall,1997; 36: 807 [11] Chen R, Zhao P, Dong B, Gao S J, Shen B L,TU M J.Chin J Non-Met, 1998; 8(1): 181(陈 睿,赵 平,董 斌,高升吉,沈保罗,涂明旌.中国有色金属学报,1998;8(1):181) [12] Vyletel G M, Aken D C.Mater Trans,1995;A26:3155 [13] Stefano S, Lorenzo P.Metall Mater Trans,1995; A26:2745 [14] Liu P L. Ph D Thesis, Institute of Metal Research ofAcademia Sinica, 1997. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|