| 定向凝固NiAl-Cr(Mo)-Hf合金微观结构的电子显微学研究 |
| 陈玉喜 崔传勇 贺连龙 郭建亭 李斗星 |
| 中国科学院研究所固体原子开放研究实验室;沈阳 110015 |
|
引用本文:
陈玉喜; 崔传勇; 贺连龙; 郭建亭; 李斗星 . 定向凝固NiAl-Cr(Mo)-Hf合金微观结构的电子显微学研究[J]. 金属学报, 1999, 35(9): 897-901 .
[1] Cline H E, Walter J L. Lifshin E, Rudded R R. Metatl Trans,1971:2:189 [2] Walter J L, Cline H E Metall Trans, 1970: 1: 1221 [3] Cline H E, Walter J L. Metall Trans, 1970;1:2907 [4] Oh I K,Horita Z.Nemoto M. Mater Sci Eng,1997;A239-240:472 [5] Locci I E.Dickerson R M,Garg A、Noebe R D、Whitten-betger J D, Nathal M V、 Darolia R J Mater Res,1996: 11:3024 [6] Garg A, Noebe R D,Darolia R. Acta Mater, 1996;44: 2809 [7] Yang J M.Jeng S M,Bain K,Amato A.Acta Mater,1997;45:295 [8] Takeyama M. Liu C T J Mater Res. 1990;5: 1189 [9] Cline H E, Walter J L, Koch E F、 Osika L M. Acta Metall,1971; 19: 405 [10] Chen X F. Johson D R Noebe R D, Oliver B F. J MaterRes, 1995;10:1159 [11] Johnson D R,Chen X F,Oliver B F.Noebe R D,Whitten-berger J D.Intermetallics,1995;3:99 |
|