| Ni3Al基复合材料的组织与性能 |
| 冯涤 叶武俊 |
| 钢铁研究总院; 北京 100081 |
|
引用本文:
冯涤; 叶武俊 . Ni3Al基复合材料的组织与性能[J]. 金属学报, 1999, 35(1): 86-88 .
| 1]SikkaVK,MavityJT.MaterSciEng,1992;A153:172[2]JohnsonML,MikkolaDE,WrightRN.Intermetalics,1995;3:389[3]HanGW,FengD,YeWJ.HighTechnolLet,1993;(10):13(韩光玮,冯涤,叶武俊.高技术通讯,1993;(10):13)[4]YeWJ,FengD,HanGW.JIronStelRes,1997;9(Suppl.):231(叶武俊,冯涤,韩光玮.钢铁研究学报,1997;9(增刊):231)[5]YeWJ,FengD.Report,CentralIronandSteelResearchInstitute,Beijing,1998(叶武俊,冯涤.钢铁研究总院内部资料,北京,1988)[6]YeWJ,FengD.‘85’FinalResearchReport,Beijing:CentralIronandStelResearchInstitute,Beijing,1996(叶武俊,冯涤.863计划‘85’最终科技报告,钢铁研究总院,北京,1996)[7]DuanCG.SiltAbrasiveErosionofHydraulicTurbine.Beijing:TsinghuaUniversityPres,1981:169(段昌国.水轮机沙粒磨损.北京:清华大学出版社,1981:169) |
|