| Zn—48.48Al—1.65Cu—0.03Mg合金液表面氧化膜微细特性 |
| 陈云贵;涂铭旌 |
| 四川联合大学金属材料系;成都;610065;四川联合大学金属材料系;成都;610065 |
|
| CHAJRACTERISTICS OF OXIDE FORMED ON THE SURFACE OF Zn-48.48Al-1.65Cu-0.03Mg MELT |
| CHEN Yunwi; TU Mingjing(Department of Metal Materials; Sichuan Union University; Chengdu 610065)Correspondent: CHEN Yungui; associate professor Tel.(028)5405701; Fax:(028)5220670 |
引用本文:
陈云贵;涂铭旌. Zn—48.48Al—1.65Cu—0.03Mg合金液表面氧化膜微细特性[J]. 金属学报, 1998, 34(6): 621-626.
,
.
CHAJRACTERISTICS OF OXIDE FORMED ON THE SURFACE OF Zn-48.48Al-1.65Cu-0.03Mg MELT[J]. Acta Metall Sin, 1998, 34(6): 621-626.
1 中国机械工程学会铸造专业学会 铸造手册-铸造非铁合金,第3卷北京:机械工业出版社,1993:24(The Foudry Institute of Chinese Mechanical Engineering .Foundry Handbooks -Foundry Nonfeerous Alloys ,V.S. Beijing: Mechanical Industry Pres 1993: 24) 2 山下次郎,国井真澄.铸造工学,1996;(3)68:249(Jiro Yamashita, Masumi Kunni.J Jpn Foundry Soc. 1996;(3)68: 249) 3 Mahanti R K, Lal K, Sivaramakrisbnan C S, Mohanty O N, Jian K B. The Thansactions of AmericanFoundryman Society, 1992; 100: 857 4 PH1 5300 Instrument Manual . USA: Perkin—Elmer Corporation, 1989: 520 5 Wagner C D, Riggs W M, Davis L E, Mouldef J F, Muilehberg G E. Handbook of X-ray Photoelectron Spetroacopy. USA: Perkin-Elmet Corpoetatiorp Phpoical Electronic Division, 1978: 50 6 Power Diffraction File.USA:Inernational Centre for Diffraction Data ,1989:5-0669,21—1486,21—1152 7 樱并良文,小泉光惠等著,陈俊彦,王余君译.新型陶瓷-材料及应用.北京:中国建筑工业出版社,1983:77(Sakurai Yoshibumi, Koisumi Mitsuye et al、 Advanced Cermaic-materials and Applications Beijing ThePress of China Building and Construction Induaryt 1983: 77) 8 梁英教,车荫昌 无机物热力学数据手册.沈阳:东北大学出版社.1993:450—478(Liang Y J, Che Y C.Thermodynamic Data Handbook of inorganic Substances .Shenyand :NortheasternUniversity Press, 1993: 450) 9 吴清辉.表面化学与多相催化北京:化学工业出版社,1991:87(Wu QH.Surface Chemistry and heterogeneous Catahysis Beijing :Chemistry Industry Press ,,1991:87) 10 West R C, Astle M Jt Beyer W H. CRC Hondbok of Chemistry and Physica,69th Edition. USA: CRC Press, Inc. 1988: F-20 11 陈鸿海 金属腐蚀学.北京:北京理工大学出版社,1995:34(Chen H H. Metallic Corrosion .Beijing .The Press of Beijing Institute fo Technology 1995: 34) |
|