| 贝氏体三维形态及组织演化 |
| 方鸿生;薄祥正;王家军;徐宁 |
| 清华大学材料科学与工程系;北京;100084;清华大学材料科学与工程系;北京;100084;清华大学材料科学与工程系;北京;100084;清华大学材料科学与工程系;北京;100084 |
|
| THREE DIMENSIONAL MORPHOLOGY AND MICROSTRUCTURAL EVOLUTION OF BAINITE |
| FANG Hongsheng; BO Xiangzheng; WANG Jiajun; XU Ning(Deperment of Materials Science & Engineering; Tsinghua University; Beijing 100084)Correspondent : BO Xiangzheag Fas:(010)62771160; Tel: (010)62782361;E-mail: fhsdms tsinghua edu .cn |
引用本文:
方鸿生;薄祥正;王家军;徐宁. 贝氏体三维形态及组织演化[J]. 金属学报, 1998, 34(6): 579-585.
,
,
,
.
THREE DIMENSIONAL MORPHOLOGY AND MICROSTRUCTURAL EVOLUTION OF BAINITE[J]. Acta Metall Sin, 1998, 34(6): 579-585.
1 Oblak J M, Goodenow R H, Hehemann R F. Trans AIME, 1964; 230: 258 2 Stinivasan G R, Wayman C M. Acta Metall 1968; 16(6): 621 3 Fang H S, Wang J J, Yang Z G, Li C M, Deng X R, Zheng Y K, Yan J J, Yu H B, Li Z G, Huang G. Prog Nat Sci,1994; 4(2):182 4 Wang J J, Fang H S, Yang Z G, Zheng Y K. ISIJ Int, 1995; 35(8): 992 5 方鸿生,杨志刚,王家军,郑蔡康.金属学报,1995;31:A387(Fang H S, Yang Z G, Wang J J, and Zheng Y K, Acta Metall Sin, 1995; 31: A387)6 方鸿生,王家军.金属学报,1994;30:A491(Fang H S, Wang J J. Acta Metall Sin, 1994; 30: A491) 7 方鸿生,王家军.郑燕康,杨志刚.金属学报,1993;29:A445(Fang H S, Wang J J, Zheng Y K, Yang Z G. Acta Mentall Sin 1993; 29: A445) 8 方鸿生,王家军,杨志刚.钢铁研究学报,1997;9(5):45(Fang H S, Wang J J, Yang Z G.J Iron Steel Rea, 1997; 9(5): 45) |
|